Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of INNOPRENE 1450 N - TPE - Kumho Polychem

Material Data Center offers the following functions for INNOPRENE 1450 N:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Innoprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la traction 4.9 MPa ISO 37
Déformation rémanente en compression à 70 °C, 24h 31 % ISO 815
Résistance à la déchirure 24.5 kN/m ISO 34-1
Dureté Shore A 46 - ISO 7619-1
ASTM Data
Module à 100% allongement 1.47 MPa ASTM D 412
Dureté A Shore 46 - ASTM D 2240
Résistance au déchirement 24.5 kN/m ASTM D 624
Compression rémanente, 22 hr @ 158 °F 31 % ASTM D 395
Module de traction 4.9 MPa ASTM D 412
Propriétés diversesValeurUnitéNorme du test
Masse volumique 950 kg/m³ ISO 1183
Densité 950 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 85 °C -
Pré-séchage - temps 3 h -
Température de la matière fondue 190 - 230 °C -
Température du moule 10 - 60 °C -
Zone 1 160 - 180 °C -
Zone 2 180 - 200 °C -
Zone 3 200 °C -
Température de la buse 200 - 220 °C -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Pré-séchage - température 85 °C -
Pré-séchage - temps 3 h -
Température de la matière fondue 190 - 230 °C -
Température - Zone d'alimentation 160 - 170 °C -
Zone 1 180 - 200 °C -
Zone 2 180 - 200 °C -
Zone 3 180 - 200 °C -
Température de la buse 180 - 210 °C -
Caractéristiques
Transformation
Moulage par injection, Extrusion de tubes, Extrusion de profilés, Extrusion de plaques, Extrusion de cable, Soufflage, Calandrage
Conditionnement
Granulés, Couleurs naturelles
Propriétés spéciales
Stabilisé aux intempéries, Stabilisé à la chaleur
Caractéristiques
Résistance à la fatigue
Résistance Chimique
Résistance chimique générale, Résistance à l’ozone
Applications
General Purpose
Disponibilité régionale
Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com