Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Inzea® F19 HT - (PLA+PSAC) - Nurel S.A.

Material Data Center offers the following functions for Inzea® F19 HT:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Inzea datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
more information can be found in the following table
Rilsamid® Chemical Resistance
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 5 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 70 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Moisture Content 0.3 % -
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Module en traction, parallèle 2700 MPa ISO 527-3
Contrainte à la rupture, parallèle 40 MPa ISO 527-3
Déformation maximale, parallèle 100 % ISO 527-3
Résistance au déchirement pantalon, normal 9 N/mm ISO 6383-1
Type d'extrusion soufflage - -
Epaisseur des eprouvettes 0.05 mm -
Caractéristiques
Transformation
Extrusion (autres), Thermoformage
Propriétés spéciales
Transparent
Certifications
Contient des ressources renouvelables, Biodégradables, Contact alimentaire, Compostable ISO 13432 (producteur), Compostable ISO 13432 (certificat)
Disponibilité régionale
Europe, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.