Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of K-Resin® KR38 - SB - INEOS Styrolution

Material Data Center offers the following functions for K-Resin® KR38:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other K-Resin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
K-Resin® KR38 alone or in blends, can be easily processed by extrusion and gives thermoformed parts with excellent detail on fast production cycles. The favorable economics of K-Resin SBC, along with high productivity, have made possible tough clear disposable drinking cups, lids, IC carrier tape and other packaging applications.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9 cm³/10min ISO 1133
Température 200 °C -
Charge 5 kg -
Indice de fluidité, MFI 9 g/10min ISO 1133
Température 200 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 900 MPa ISO 527
Contrainte d'écoulement 16.2 MPa ISO 527
Déformation à la rupture >50 % ISO 527
Module de flexion, 23°C 1360 MPa ISO 178
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 50 kJ/m² ISO 179/1eA
Dureté Shore D 56 - ISO 7619-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 55 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 73 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 50 °C ISO 306
ASTM Data
Vicat température 74.4 °C ASTM D 1525
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Lumière á Transmittance 92 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.07 % Sim. to ISO 62
Masse volumique 1000 kg/m³ ISO 1183
Caractéristiques
Transformation
Extrusion de plaques, Soufflage, Thermoformage
Conditionnement
Granulés
Propriétés spéciales
Transparent
Caractéristiques
Mélange de résine, High Gloss, Copolymère
Certifications
Contact avec l'eau potable
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Autres informations
Moulages par injection
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com