Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KDL1040 - PA66-GF40 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KDL1040:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.5 % ISO 294-4, 2577
ASTM Data
Retrait au moulage , parallèle 0.0055 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la traction 236 MPa ISO 527
Module de flexion 10000 MPa ISO 178
Résistance à la flexion 334 MPa ISO 178
Résistance au choc Charpy, +23°C 75 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 26 kJ/m² ISO 179/1eA
Dureté Rockwell R 122 - ISO 2039-2
ASTM Data
Module en traction 235 MPa ASTM D 638
Module de traction 14300 MPa ASTM D 638
Module de flexion 12500 MPa ASTM D 790
Résistance à la flexion 330 MPa ASTM D 790
Dureté Rockwell R 122 - ASTM D 785
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 262 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 254 °C ISO 75-1/-2
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
ASTM Data
UL 94 inflammabilité HB - UL 94
DTUL à 264 psi 254 °C ASTM D 648
Température de fusion 262 °C ASTM D 3418
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 3.8 - IEC 62631-2-1
Facteur de pertes, 1MHz 0.02 E-4 IEC 62631-2-1
Résistivité transversale 1E15 Ohm*m IEC 62631-3-1
Rigidité diélectrique 22 kV/mm IEC 60243-1
ASTM Data
Rigidité diélectrique, peu de temps 35 kV/mm ASTM D 149
Facteur de dissipation diélectrique, 1 MHz 0.01 - ASTM D 150
Constante diélectrique, 1 MHz 3.7 - ASTM D 150
Résistance volumique 1E15 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1450 kg/m³ ISO 1183
Absorption d’eau, 24hr 0.5 % ASTM D 570
Densité 1450 kg/m³ ASTM D 792
Caractéristiques
Propriétés spéciales
Modifié choc
Caractéristiques
Résistance au fluage, Long fiber reinforced
Applications
Automobile
Disponibilité régionale
Amérique du nord, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.