Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar® 460 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar® 460:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Kynar® resins are fluorinated thermoplastic homopolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties. This product is NSF/ANSI/CAN 61 certified. 

Kynar® 460 resin is a standard grade of granules for extrusion of tubes, cables and plaques, compression and transfer molding.


Main applications:
  • corrosion protection in the chemical industry
  • coating (painting, co-extrusion)
  • off shore
  • wire and cable
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 5.6 cm³/10min ISO 1133
Température 230 °C -
Charge 21.6 kg -
Retrait au moulage, parallèle 2.0 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 2.0 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1400 MPa ISO 527
Contrainte d'écoulement 42 MPa ISO 527
Déformation au seuil d'écoulement 13 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 161 °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min -40 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 85 °C ISO 75-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Aptitude à l'allumage 43 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 9 - IEC 62631-2-1
Permittivité relative, 1MHz 6.7 - IEC 62631-2-1
Facteur de pertes, 100Hz 1300 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 700 E-4 IEC 62631-2-1
Résistivité transversale 2E12 Ohm*m IEC 62631-3-1
Rigidité diélectrique 63 kV/mm IEC 60243-1
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.04 % Sim. to ISO 62
Masse volumique 1760 kg/m³ ISO 1183
Caractéristiques
Transformation
Extrusion de profilés, Extrusion (autres)
Conditionnement
Granulés
Caractéristiques
Homopolymère
Disponibilité régionale
Résistance Chimique
Acides
Acide acétique (masse en 5%) (23°C)
Acide citrique (masse en 10%) (23°C)
Acide lactique (masse en 10%) (23°C)
Acide chlorhydrique (masse en 36%) (23°C)
Acide nitrique (masse en 40%) (23°C)
Acide sulfurique (masse en 38%) (23°C)
Acide sulfurique (masse en 5%) (23°C)
Acide chromique (masse en 40%) (23°C)
Bases
Hydroxyde de soude (masse en 35%) (23°C)
Hydroxyde de soude (masse en 1%) (23°C)
Hydroxyde d'ammoniaque (masse en 10%) (23°C)
Alcool
Isopropanol (23°C)
Méthanol (23°C)
Ethanol (23°C)
Hydrocarbures
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Cetones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Huiles minérales
Huile moteur multigrade SAE 10W40 (23°C)
Huile moteur multigrade SAE 10W40 (130°C)
Huile engrenage hypoide SAE 80/90 (130°C)
Huile d'isolation (23°C)
Carburants standards
ISO 1817 Liquide 1 (60°C)
ISO 1817 Liquide 2 (60°C)
ISO 1817 Liquide 3 (60°C)
ISO 1817 Liquide 4 (60°C)
Carburant stand. sans alcool (de pref. ISO 1817 liquide C) (23°C)
Carburant stand. avec alcool (de pref. ISO 1817 Liquid 4) (23°C)
Gasoil (pref. ISO 1817 liquide F) (23°C)
Gasoil (pref. ISO 1817 liquide F) (90°C)
Gasoil (pref. ISO 1817 liquide F) (>90°C)
Selts
Chlorure de sodium (masse en 10%) (23°C)
Hypochlorite de soude (masse en 10%) (23°C)
Carbonate de soude (masse en 20%) (23°C)
Carbonate de soude (masse en 2%) (23°C)
Chlorure de zinc (masse en 50%) (23°C)
Autres
Acétate d'éthyle (23°C)
Peroxyde d'hydrogene (23°C)
Ethylene glycol (108°C)
L'eau (23°C)
L'eau déionisée (90°C)
Phénol (masse en 5%) (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.