Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of LUPOY GN2101FB - PC-GF10 - LG Chem
Material Data Center offers the following functions for LUPOY GN2101FB:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
ISO Data |
Indice de fluidité, MFI |
8.3 |
g/10min |
ISO 1133 |
Température |
300 |
°C |
- |
Charge |
1.2 |
kg |
- |
Retrait au moulage, parallèle |
0.6 |
% |
ISO 294-4, 2577 |
Retrait au moulage, perpendiculaire |
0.5 |
% |
ISO 294-4, 2577 |
ASTM Data |
Indice de fluidité, MFI |
8.3 |
g/10min |
ASTM D 1238 |
Température |
300 |
°C |
- |
Charge |
1.2 |
kg |
- |
Retrait au moulage , parallèle |
0.006 |
mm/mm |
ASTM D 955 |
Retrait au moulage, perpendiculaire |
0.005 |
mm/mm |
ASTM D 955 |
Propriétés mécaniques | Valeur | Unité | Norme du test |
ISO Data |
Module en traction |
3620 |
MPa |
ISO 527 |
Contrainte d'écoulement |
60 |
MPa |
ISO 527 |
Déformation au seuil d'écoulement |
5 |
% |
ISO 527 |
Contrainte à la rupture |
45 |
MPa |
ISO 527 |
Déformation à la rupture |
10 |
% |
ISO 527 |
Module de flexion, 23°C |
3620 |
MPa |
ISO 178 |
Résistance à la flexion |
105 |
MPa |
ISO 178 |
Résistance au choc Charpy (entaillé), +23°C |
6[1] |
kJ/m² |
ISO 179/1eA |
Résistance au choc Charpy (entaillé), -30°C |
6[1] |
kJ/m² |
ISO 179/1eA |
Résistance au choc Izod avec entaille, +23°C |
6[1] |
kJ/m² |
ISO 180/1A |
Résistance au choc Izod avec entaille |
6[1] |
kJ/m² |
ISO 180/1A |
Température |
-40 |
°C |
- |
Dureté Rockwell |
R 122 |
- |
ISO 2039-2 |
ASTM Data |
Module en traction |
3835 |
MPa |
ASTM D 638 |
Module de traction d’élasticité |
63.8 |
MPa |
ASTM D 638 |
Résistance de traction à la rupture |
48 |
MPa |
ASTM D 638 |
Allongement d’élasticité |
5 |
% |
ASTM D 638 |
Allongement à la rupture |
15 |
% |
ASTM D 638 |
Module de flexion |
3475 |
MPa |
ASTM D 790 |
Résistance à la flexion |
105 |
MPa |
ASTM D 790 |
Dureté Rockwell |
R 122 |
- |
ASTM D 785 |
Izod choc avec entaille, 1/8 in |
88.3 |
J/m |
ASTM D 256 |
Izod choc avec entaille, 1/4 in |
68.7 |
J/m |
ASTM D 256 |
Izod choc avec entaille, bas température |
58.9 |
J/m |
ASTM D 256 |
Température |
-30 |
°C |
- |
Propriétés thermiques | Valeur | Unité | Norme du test |
ISO Data |
Température de fléchissement s/chrg, 1.80 MPa |
121 |
°C |
ISO 75-1/-2 |
Température de fléchissement s/chrg, 0.45 MPa |
132 |
°C |
ISO 75-1/-2 |
Température de ramolliss. Vicat, B |
142 |
°C |
ISO 306 |
Coeffic. de dilatation therm. linéique, parallèle |
44 |
E-6/K |
ISO 11359-1/-2 |
Coeffic. de dilatation therm. linéique, perpend. |
88 |
E-6/K |
ISO 11359-1/-2 |
Inflammabilité ep. nom. 1.5 mm |
V-0 |
class |
IEC 60695-11-10 |
Epaisseur de l'éprouvette |
1.5 |
mm |
- |
Inflammabilité 5V pr. épaisseur h |
5VA |
class |
IEC 60695-11-20 |
Epaisseur de l'éprouvette |
3.0 |
mm |
- |
ASTM Data |
UL 94 inflammabilité |
V-0 |
- |
UL 94 |
Épaisseur testée |
1.5 |
mm |
- |
coefficient de dilatation thermique, long. |
44 |
E-6/K |
ASTM D 696 |
Coefficient de dilatation thermique, trav. |
88 |
E-6/K |
ASTM D 696 |
DTUL à 66 psi |
133[2] |
°C |
ASTM D 648 |
DTUL à 264 psi |
127[2] |
°C |
ASTM D 648 |
Vicat température |
136 |
°C |
ASTM D 1525 |
Propriétés électriques | Valeur | Unité | Norme du test |
ISO Data |
Résistivité transversale |
1E15 |
Ohm*m |
IEC 62631-3-1 |
Résistivité superficielle |
1E15 |
Ohm |
IEC 62631-3-2 |
Indice de résistance au cheminement |
212 |
- |
IEC 60112 |
ASTM Data |
Rigidité diélectrique, peu de temps |
20 |
kV/mm |
ASTM D 149 |
Résistance de la surface |
1E15 |
Ohm |
ASTM D 257 |
Résistance volumique |
1E17 |
Ohm*cm |
ASTM D 257 |
Propriétés diverses | Valeur | Unité | Norme du test |
Absorption d'humidité |
0.2 |
% |
Sim. to ISO 62 |
Masse volumique |
1250 |
kg/m³ |
ISO 1183 |
Densité |
1250 |
kg/m³ |
ASTM D 792 |
Recommandations pour la transformation Moulage par injection | Valeur | Unité | Norme du test |
Pré-séchage - température |
100 - 120 |
°C |
- |
Pré-séchage - temps |
3 - 5 |
h |
- |
L'humidité de traitement |
≤0.02 |
% |
- |
Température de la matière fondue |
300 - 340 |
°C |
- |
Température du moule |
90 - 120 |
°C |
- |
Zone 1 |
270 - 300 |
°C |
- |
Zone 2 |
280 - 310 |
°C |
- |
Zone 3 |
290 - 330 |
°C |
- |
Température de la buse |
290 - 330 |
°C |
- |
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Ignifugé, Sans halogène
Applications
General Purpose
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.