Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY GN5007FM - (PC+ABS) - LG Chem

Material Data Center offers the following functions for LUPOY GN5007FM:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 5.4 g/10min ISO 1133
Température 250 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.7 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 % ISO 294-4, 2577
ASTM Data
Indice de fluidité, MFI 5.4 g/10min ASTM D 1238
Température 250 °C -
Charge 2.16 kg -
Retrait au moulage , parallèle 0.0065 mm/mm ASTM D 955
Retrait au moulage, perpendiculaire 0.0075 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2130 MPa ISO 527
Contrainte d'écoulement 61 MPa ISO 527
Déformation au seuil d'écoulement 6.4 % ISO 527
Contrainte à la rupture 61 MPa ISO 527
Déformation à la rupture 100 % ISO 527
Module de flexion, 23°C 2170 MPa ISO 178
Résistance à la flexion 90 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 55[1] kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 12[1] kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 33[1] kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 11[1] kJ/m² ISO 180/1A
Température -40 °C -
Dureté Rockwell R 118 - ISO 2039-2
ASTM Data
Module en traction 2077 MPa ASTM D 638
Module de traction d’élasticité 60.8 MPa ASTM D 638
Résistance de traction à la rupture 64.7 MPa ASTM D 638
Allongement d’élasticité 6.6 % ASTM D 638
Allongement à la rupture 122 % ASTM D 638
Module de flexion 2256 MPa ASTM D 790
Résistance à la flexion 98.1 MPa ASTM D 790
Dureté Rockwell R 118 - ASTM D 785
Izod choc avec entaille, 1/8 in 746 J/m ASTM D 256
Izod choc avec entaille, 1/4 in 108 J/m ASTM D 256
Izod choc avec entaille, bas température 108 J/m ASTM D 256
Température -30 °C -
1: 4 mm
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 110 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 134 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 130 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 85 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 77 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
ASTM Data
UL 94 inflammabilité V-0 - UL 94
Épaisseur testée 1.5 mm -
coefficient de dilatation thermique, long. 85 E-6/K ASTM D 696
Coefficient de dilatation thermique, trav. 77 E-6/K ASTM D 696
DTUL à 66 psi 136[2] °C ASTM D 648
DTUL à 264 psi 120[2] °C ASTM D 648
Vicat température 141 °C ASTM D 1525
2: 6.4 mm
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Résistivité transversale 1E15 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E15 Ohm IEC 62631-3-2
Indice de résistance au cheminement 212 - IEC 60112
ASTM Data
Rigidité diélectrique, peu de temps 18 kV/mm ASTM D 149
Résistance de la surface 1E15 Ohm ASTM D 257
Résistance volumique 1E17 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.2 % Sim. to ISO 62
Masse volumique 1190 kg/m³ ISO 1183
Densité 1190 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 100 °C -
Pré-séchage - temps 3 - 5 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 270 - 290 °C -
Température du moule 80 - 120 °C -
Zone 1 260 - 270 °C -
Zone 2 270 - 280 °C -
Zone 3 280 - 290 °C -
Température de la buse 300 - 320 °C -
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Ignifugé, Sans halogène
Applications
Automobile, Électrotechnique et électrique, General Purpose
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.