Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® 358N Crystal Clear - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® 358N Crystal Clear:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Grade for application where highest transparency and low natural colour combined with easy-flow is required.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 22 cm³/10min ISO 1133
Température 220 °C -
Charge 10 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3700 MPa ISO 527
Contrainte à la rupture 72 MPa ISO 527
Déformation à la rupture 3 % ISO 527
Module de fluage en traction, 1h 3500 MPa ISO 899-1
Module de fluage en traction, 1000h 2800 MPa ISO 899-1
Résistance au choc Charpy, +23°C 16 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 16 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 2 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 86 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 99 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 106 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 70 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Yellow Card disponible oui - -
Aptitude à l'allumage 18 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3 - IEC 62631-2-1
Permittivité relative, 1MHz 2.7 - IEC 62631-2-1
Facteur de pertes, 100Hz 40 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 70 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle >1E15 Ohm IEC 62631-3-2
Indice de résistance au cheminement 400 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.2 % Sim. to ISO 62
Masse volumique 1080 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 230 °C ISO 294
Injection, température du moule 50 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 220 - 260 °C -
Température du moule 40 - 80 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Contrainte de cisaillement / Vit. de cisaillement , Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Contrainte / Déformation , Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Module sécant / Déformation , Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 23°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Module de fluage / Temps 23°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Courbe de fluage 23°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 40°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Module de fluage / Temps 40°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Courbe de fluage 40°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 60°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Module de fluage / Temps 60°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Courbe de fluage 60°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 80°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Module de fluage / Temps 80°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Courbe de fluage 80°C, Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Volume spécifique (pvT) , Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Module de traction / Température , Luran® 358N Crystal Clear, SAN, INEOS Styrolution
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Transparent
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 220 - 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.