Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NOPLA® KE101 - (PEN+PET) - Kolon Industries

Material Data Center offers the following functions for NOPLA® KE101:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Nopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 15 g/10min ISO 1133
Température 275 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.6 % ISO 294-4, 2577
ASTM Data
Indice de fluidité, MFI 8.1 g/10min ASTM D 1238
Température 260 °C -
Charge 1.05 kg -
Retrait au moulage , parallèle 0.005 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la traction 60 MPa ISO 527
Module de flexion, 23°C 2900 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 3.5 kJ/m² ISO 179/1eA
Dureté Rockwell R 88 - ISO 2039-2
ASTM Data
Module de traction 60 MPa ASTM D 638
Module de flexion 2854 MPa ASTM D 790
Résistance à la flexion 92 MPa ASTM D 790
Dureté Rockwell R 88 - ASTM D 785
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 230 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 0.45 MPa 75 °C ISO 75-1/-2
Inflammabilité pr. épaisseur h V-2 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
ASTM Data
UL 94 inflammabilité V-2 - UL 94
Épaisseur testée 0.8 mm -
coefficient de dilatation thermique, long. 60 E-6/K ASTM D 696
DTUL à 66 psi 77 °C ASTM D 648
Température de fusion 234 °C ASTM D 3418
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 1 % ASTM D 1003
Lumière á Transmittance 85 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1330 kg/m³ ISO 1183
Densité 1330 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 140 - 160 °C -
Pré-séchage - temps 3 - 6 h -
L'humidité de traitement ≤0.08 % -
Température du moule 30 - 80 °C -
Zone 1 160 - 210 °C -
Zone 2 200 - 240 °C -
Zone 3 220 - 250 °C -
Température de la buse 230 - 265 °C -
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Transparent
Caractéristiques
Copolymère
Disponibilité régionale
Amérique du nord, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.