Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® H701 - ABS - INEOS Styrolution

Material Data Center offers the following functions for Novodur® H701:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
medium heat resistance, high impact strength
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 8 cm³/10min ISO 1133
Température 220 °C -
Charge 10 kg -
Densité du fondu 885 kg/m³ -
Conductivité thermique du fondu 0.127 W/(m K) -
Chaleur spécifique du fondu 1800 J/(kg K) -
Température d'éjection 85 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2100 MPa ISO 527
Contrainte d'écoulement 41 MPa ISO 527
Déformation au seuil d'écoulement 2.7 % ISO 527
Résistance au choc Charpy, +23°C 180 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 120 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 24 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 13 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 99 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 105 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 103 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 90 E-6/K ISO 11359-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.1 - IEC 62631-2-1
Permittivité relative, 1MHz 2.9 - IEC 62631-2-1
Facteur de pertes, 100Hz 50 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 90 E-4 IEC 62631-2-1
Rigidité diélectrique 33 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1040 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 240 °C ISO 294
Injection, température du moule 70 °C ISO 294
Injection, vitesse d'injection 240 mm/s ISO 294
Fonctions
Viscosité / Vitesse de cisaillement , Novodur® H701, ABS, INEOS Styrolution
Contrainte de cisaillement / Vit. de cisaillement , Novodur® H701, ABS, INEOS Styrolution
Contrainte / Déformation , Novodur® H701, ABS, INEOS Styrolution
Module sécant / Déformation , Novodur® H701, ABS, INEOS Styrolution
Volume spécifique (pvT) , Novodur® H701, ABS, INEOS Styrolution
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Disponibilité régionale
Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.