Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 2533 SD 02 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 2533 SD 02:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Polyether block amide Pebax® 2533 SD 02 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This SD grade is heat and UV stabilized and contains mould release additive.


Main applications:
  • Flexible injected parts
  • Silent gears


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 12 / 10 MPa ISO 527
Contrainte pr. une déform. de 50% 3 / 3 MPa ISO 527
Déformation à la rupture >50 / >50 % ISO 527
Contrainte à 10% de déformation 1 / * MPa ISO 527
Contrainte à 100% de déformation 4 / * MPa ISO 527
Contrainte à la rupture TPE 32 / * MPa ISO 527
Déformation à la rupture TPE >300 / * % ISO 527
Déformation rémanente en compression à 23 °C, 24h 19 / * % ISO 815
Résistance à la déchirure 44 / * kN/m ISO 34-1
Résistance à l'abrasion 130 / * mm³ ISO 4649
Dureté Shore A 74 / * - ISO 7619-1
Dureté Shore D 22 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 134 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min -65 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 0.45 MPa 42 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 200 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 6 / - - IEC 62631-2-1
Permittivité relative, 1MHz 6 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 552 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 378 / - E-4 IEC 62631-2-1
Résistivité transversale 1.3E10 / - Ohm*m IEC 62631-3-1
Résistivité superficielle * / 3E12 Ohm IEC 62631-3-2
Rigidité diélectrique 36 / - kV/mm IEC 60243-1
Indice de résistance au cheminement * / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.2 / * % Sim. to ISO 62
Absorption d'humidité 0.4 / * % Sim. to ISO 62
Masse volumique 1000 / 1000 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Pebax® 2533 SD 02, TPA, ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Pebax® 2533 SD 02, TPA, ARKEMA
Contrainte / Déformation , Pebax® 2533 SD 02 (sec), TPA, ARKEMA
Module sécant / Déformation , Pebax® 2533 SD 02 (sec), TPA, ARKEMA
Contrainte / Déformation (isochrone) 23°C, Pebax® 2533 SD 02 (sec), TPA, ARKEMA
Module de fluage / Temps 23°C, Pebax® 2533 SD 02 (sec), TPA, ARKEMA
Courbe de fluage 23°C, Pebax® 2533 SD 02 (sec), TPA, ARKEMA
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion (autres), Moulage par transfert, Coulage, Thermoformage
Conditionnement
Granulés
Additifs
Lubrifiant, Agent antiadhérent
Propriétés spéciales
Galvanisable, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 180°C / 210°C / 240°C.
- Typical mold temperature : 10 – 30°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 55-65°C.

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com