Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 5533 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 5533 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Polyether block amide Pebax® 5533 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This SP grade has been developed to be heat and UV resistant.


Main applications:
  • Athletic foot wear components
  • Ski shoes
  • High performance power trasmission belts


Packaging:

This grade is delivered dried in sealed packaging (20 or 25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 170 / 161 MPa ISO 527
Contrainte d'écoulement 12 / 12 MPa ISO 527
Déformation au seuil d'écoulement 25 / 25 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Contrainte à 10% de déformation 10 / * MPa ISO 527
Contrainte à 100% de déformation 14 / * MPa ISO 527
Contrainte à la rupture TPE 52 / * MPa ISO 527
Déformation à la rupture TPE >300 / * % ISO 527
Déformation rémanente en compression à 23 °C, 24h 43 / * % ISO 815
Résistance à la déchirure 106 / * kN/m ISO 34-1
Résistance à l'abrasion 47 / * mm³ ISO 4649
Dureté Shore D 50 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 159 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 0.45 MPa 66 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 66 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 170 / * E-6/K ISO 11359-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 9 / - - IEC 62631-2-1
Permittivité relative, 1MHz 5 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 1110 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 1020 / - E-4 IEC 62631-2-1
Résistivité transversale 3.2E11 / - Ohm*m IEC 62631-3-1
Résistivité superficielle * / 3E12 Ohm IEC 62631-3-2
Rigidité diélectrique 38.5 / - kV/mm IEC 60243-1
Indice de résistance au cheminement * / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.2 / * % Sim. to ISO 62
Absorption d'humidité 0.6 / * % Sim. to ISO 62
Masse volumique 1010 / 1010 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 65 - 75 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 200 - 270 °C -
Température du moule 25 - 60 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Pebax® 5533 SP 01, TPA, ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Pebax® 5533 SP 01, TPA, ARKEMA
Contrainte / Déformation , Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Contrainte / Déformation , Pebax® 5533 SP 01 (cond.), TPA, ARKEMA
Module sécant / Déformation , Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Module sécant / Déformation , Pebax® 5533 SP 01 (cond.), TPA, ARKEMA
Contrainte / Déformation (isochrone) 23°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Module de fluage / Temps 23°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Courbe de fluage 23°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Contrainte / Déformation (isochrone) 40°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Module de fluage / Temps 40°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Courbe de fluage 40°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Contrainte / Déformation (isochrone) 60°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Module de fluage / Temps 60°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Courbe de fluage 60°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Contrainte / Déformation (isochrone) 80°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Module de fluage / Temps 80°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Courbe de fluage 80°C, Pebax® 5533 SP 01 (sec), TPA, ARKEMA
Volume spécifique (pvT) , Pebax® 5533 SP 01, TPA, ARKEMA
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion (autres), Moulage par transfert, Coulage, Thermoformage
Conditionnement
Granulés
Propriétés spéciales
Galvanisable, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 200°C / 240°C / 270°C.
- Typical mold temperature : 25 – 60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
Extrusion (autres)

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 220°C / 230°C
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.