Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Platamid® H 1937 Pellets - PA* - ARKEMA
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center
Platamid® H 1937 is a thermoplastic copolyamide adhesive available in pellet form for manufacture of hot melt film and webs by extrusion.
Platamid® H 1937 has good adhesion to all kinds of textile substrates based on native and synthetic fibers.
AVAILABLE GRADES
This product is available:
- dried (H 1937 TA)
PACKAGING
- Platamid® H 1937 TA is delivered in 25 kg sealed bags.
This grade is ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Caractéristiques des transformations/physiques | sec / cond | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Indice de fluidité à chaud en volume, MVR | 18 / * | cm³/10min | ISO 1133 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Température | 160 / * | °C | - | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Charge | 2.16 / * | kg | - |
Propriétés thermiques | sec / cond | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Température de fusion, 10°C/min | 102 / * | °C | ISO 11357-1/-3 |