Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Relene M26500 - (PE-LLD) - Reliance Polymers

Material Data Center offers the following functions for Relene M26500:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Relene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 50 g/10min ASTM D 1238
Température 190 °C -
Charge 2.16 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité 11.5 MPa ASTM D 638
Allongement à la rupture 600 % ASTM D 638
Module de flexion 250 MPa ASTM D 790
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
Vicat température 97 °C ASTM D 1525
Propriétés diversesValeurUnitéNorme du test
Densité 926 kg/m³ ASTM D 792
Caractéristiques
Transformation
Moulage par injection, Enduction
Conditionnement
Poudre
Caractéristiques
Bonne adhérence, Bas gauchissement
Résistance Chimique
Résistance à oxydation
Certifications
Contact alimentaire, FDA 21 CFR approbation
Applications
General Purpose
Disponibilité régionale
Europe, Asia Pacific, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.