Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESNO P302 TL - PA12-I - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESNO P302 TL:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
ISO 16396 - PA12-HIP, EGHL, C22-004

Rilsamid® AESNO P302 TL resin is a natural polyamide. 
This grade is plasticized and designed for tube extrusion.

Rilsamid® AESNO P302 TL resin falls into the PA12-HIPHL category according to DIN 73378.


Main applications:

Air brake. 
Tubing for use in motor vehicles

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. for any use above this limit, please refer to our technical services.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 13 / * cm³/10min ISO 1133
Température 235 / * °C -
Charge 5 / * kg -
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 475 / 430 MPa ISO 527
Contrainte d'écoulement 28 / 24 MPa ISO 527
Déformation au seuil d'écoulement 24 / 24 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy (entaillé), +23°C 46 / - kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 4 / 6 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 174 / * °C ISO 11357-1/-3
Coeffic. de dilatation therm. linéique, parallèle 150 / * E-6/K ISO 11359-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 1E12 / 1E12 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 7E13 Ohm IEC 62631-3-2
Rigidité diélectrique 41 / 41 kV/mm IEC 60243-1
Indice de résistance au cheminement * / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.2 / * % Sim. to ISO 62
Masse volumique 1030 / 1030 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Module de cisaillement dynamique / Température , Rilsamid® AESNO P302 TL (sec), PA12-I, ARKEMA
Contrainte / Déformation , Rilsamid® AESNO P302 TL (sec), PA12-I, ARKEMA
Module sécant / Déformation , Rilsamid® AESNO P302 TL (sec), PA12-I, ARKEMA
Contrainte / Déformation (isochrone) 23°C, Rilsamid® AESNO P302 TL (sec), PA12-I, ARKEMA
Module de fluage / Temps 23°C, Rilsamid® AESNO P302 TL (sec), PA12-I, ARKEMA
Courbe de fluage 23°C, Rilsamid® AESNO P302 TL (sec), PA12-I, ARKEMA
LTHA-Déformation à la rupture 2mm, Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés, Extrusion (autres)
Conditionnement
Granulés
Additifs
Lubrifiant, Plastifiant
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Extrusion de profilés

Processing conditions, Extrusion :

- Typical melt temperature (Min / Recommended / Max) : 200°C / 220°C / 240°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80°C.

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.