Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BESHV BLK T - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® BESHV BLK T:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Ri​lsan® BESHV BLK T is an ultra high viscosity Polyamide 11 grade specifically designed to be extruded into large diameter thick wall pipe. This grade has been specifically engineered to achieve an outstanding balance of properties for Oil & Gas piping applications. It offers a cost effective system for non-metallic corrosion free fluid transfer in critical Oil and Gas industry applications. Rilsan® Polyamide 11 is a thermoplastic material permitted by the US Department of Transportation (DOT) under the Code of Federal Regulations (CFR) Title 49, Part 192, for gas distribution piping to be installed and operated at pressures up to and including 250 psi in a design factor of 0.40.




Main applications:
  • Oil and Gas piping applications


Packaging:

This grade is delivered dried in sealed packaging ready to be processed. For best results in gas pipe extrusion, additional desiccant bed drying to maintain/achieve moisture values <0.02% is recommended.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction - / 1390 MPa ISO 527
Contrainte d'écoulement - / 42 MPa ISO 527
Déformation au seuil d'écoulement - / 5 % ISO 527
Déformation nominale à la rupture - / >50 % ISO 527
Résistance au choc Charpy (entaillé), +23°C - / 10 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C - / 11 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 189 / * °C ISO 11357-1/-3
Propriétés diversessec / condUnitéNorme du test
Masse volumique 1030 / - kg/m³ ISO 1183
Biobased content 95 % -
Caractéristiques
Transformation
Moulage par injection, Extrusion de tubes, Extrusion de profilés
Conditionnement
Granulés, Noir
Certifications
Contient des ressources renouvelables
Disponibilité régionale
Autres informations
Moulages par injection

PROCESSING CONDITIONS*

Melt Temperature: (Min / Recommended / Max) 240°C / 270°C / 290°C.

Mold: (Temperature) 20-60°C.

Drying: (Time / Temperature / Desiccant Bed Dryer) 12 hours / 80°C / -40°C.

*only necessary for bags opened for more than two hours
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.