Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SICOFLEX® S469HH - ABS - Ravago Group

Material Data Center offers the following functions for SICOFLEX® S469HH:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sicoflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 20 g/10min ISO 1133
Température 220 °C -
Charge 10 kg -
Retrait au moulage, parallèle 0.4 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 42 MPa ISO 527
Contrainte à la rupture 38 MPa ISO 527
Déformation à la rupture 10 % ISO 527
Module de flexion, 23°C 2700 MPa ISO 178
Résistance au choc Izod avec entaille, +23°C 15 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 4 kJ/m² ISO 180/1A
Température -30 °C -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 93 °C ISO 75-1/-2
Température de ramolliss. Vicat, A 106 °C ISO 306
Température de ramolliss. Vicat, B 98 °C ISO 306
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 3.2 mm -
Yellow Card disponible oui - -
Inflammabilité 5V pr. épaisseur h 5VB class IEC 60695-11-20
Epaisseur de l'éprouvette 1.6 mm -
Yellow Card disponible oui - -
Vitesse de combustion, FMVSS, épaisseur 1 mm 65 mm/min ISO 3795 (FMVSS 302)
Glow Wire Flammability Index (GWFI) 750 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.2 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1 mm -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Résistivité transversale 1E11 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E14 Ohm IEC 62631-3-2
Rigidité diélectrique 25 kV/mm IEC 60243-1
Indice de résistance au cheminement 500 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1180 kg/m³ ISO 1183
Caractéristiques
Propriétés spéciales
Ignifugé, Sans halogène, Stabilisé à la lumière, Stabilisé à la chaleur
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.