Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Stylac NF920 - ACS - Asahi Kasei

Material Data Center offers the following functions for Stylac NF920:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Stylac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 55 cm³/10min ISO 1133
Température 220 °C -
Charge 10 kg -
Indice de fluidité, MFI 59 g/10min ISO 1133
Température 220 °C -
Charge 10 kg -
ASTM Data
Retrait au moulage , parallèle 0.0055 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 44 MPa ISO 527
Module de flexion, 23°C 2550 MPa ISO 178
Résistance à la flexion 70 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 7 kJ/m² ISO 179/1eA
Dureté Rockwell R 101 - ISO 2039-2
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 74 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 88 °C ISO 306
Inflammabilité 5V pr. épaisseur h 5VA class IEC 60695-11-20
Epaisseur de l'éprouvette 2.5 mm -
ASTM Data
UL 94 inflammabilité V-0 - UL 94
Épaisseur testée 1.5 mm -
coefficient de dilatation thermique, long. 85 E-6/K ASTM D 696
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1160 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 70 - 80 °C -
Pré-séchage - temps 3 - 4 h -
Température du moule 40 - 50 °C -
Zone 1 150 - 180 °C -
Zone 2 150 - 190 °C -
Zone 3 170 - 200 °C -
Température de la buse 170 - 200 °C -
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Ignifugé
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.