Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TARFLON® LEV2200KL - PC - Idemitsu Chemicals

Material Data Center offers the following functions for TARFLON® LEV2200KL:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tarflon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 12 cm³/10min ISO 1133
Température 300 °C -
Charge 1.2 kg -
Other Standards[S]
Retrait au moulage, parallèle 0.6 % Producer Method
Retrait au moulage, perpendiculaire 0.6 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 65 MPa ISO 527
Déformation nominale à la rupture 95 % ISO 527
Module de flexion, 23°C 2300 MPa ISO 178
Résistance à la flexion 90 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 80 kJ/m² ISO 179/1eA
Dureté Rockwell R 120 - ISO 2039-2
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 125 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 65 E-6/K ISO 11359-1/-2
Inflammabilité pr. épaisseur h V-2 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.4 mm -
Propriétés électriquesValeurUnitéNorme du test
Other Standards[S]
Indice de résistance au cheminement 325 - UL 746A
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés optiquesValeurUnitéNorme du test
ISO Data
Transmittance 90[1] % ISO 13468-1, -2
ASTM Data
Indice de réfraction 1.58 - ASTM D 542
1: 3mm
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1200 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 120 °C -
Pré-séchage - temps 5 - 8 h -
Température de la matière fondue 260 - 300 °C -
Température du moule 80 - 120 °C -
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Stabilisé aux intempéries, Stabilisé à la chaleur, Transparent
Résistance Chimique
Stabilité hydrolytique
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.