Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TENAC™ MG210 - POM - Asahi Kasei

Material Data Center offers the following functions for TENAC™ MG210:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tenac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 1.5 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Indice de fluidité, MFI 1.7 g/10min ISO 1133
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3150 MPa ISO 527
Contrainte d'écoulement 75 MPa ISO 527
Déformation à la rupture 40 % ISO 527
Module de flexion, 23°C 2900 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 10 kJ/m² ISO 179/1eA
ASTM Data
Module de traction 79 MPa ASTM D 638
Allongement à la rupture 40 % ASTM D 638
Module de flexion 3040 MPa ASTM D 790
Résistance à la flexion 108 MPa ASTM D 790
Dureté Rockwell R 120 - ASTM D 785
Taber abrasion résistance 13 mg/1000 cycles ASTM D 1044
Izod choc avec entaille, 1/8 in 78 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 103 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 167 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 100 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Yellow Card disponible oui - -
ASTM Data
coefficient de dilatation thermique, long. 100 E-6/K ASTM D 696
DTUL à 66 psi 172 °C ASTM D 648
DTUL à 264 psi 136 °C ASTM D 648
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Rigidité diélectrique, peu de temps 18 kV/mm ASTM D 149
Résistance de la surface 1E17 Ohm ASTM D 257
Résistance volumique 1E16 Ohm*cm ASTM D 257
Résistance à l’arc 250 s ASTM D 495
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1420 kg/m³ ISO 1183
Absorption d’eau, 24hr 0.2 % ASTM D 570
Densité 1420 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 90 °C -
Pré-séchage - temps 3 - 4 h -
Température de la matière fondue 190 - 210 °C -
Température du moule 60 °C -
Fonctions
Contrainte / Déformation , TENAC™ MG210, POM, Asahi Kasei
Module sécant / Déformation , TENAC™ MG210, POM, Asahi Kasei
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Caractéristiques
Homopolymère
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.