Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TEREZ® PBT 6750/2 T GK 20 - PBT-GB20 - Ter Plastics

Material Data Center offers the following functions for TEREZ® PBT 6750/2 T GK 20:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Terez datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
PBT standard type with medium viscosity with 20% glass beads filled impact modified.
For all kind of injection molding parts with increased dimensional stability and tendency to warpage.
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2700 MPa ISO 527
Résistance à la traction 43 MPa ISO 527
Déformation au seuil d'écoulement 2.3 % ISO 527
Contrainte à la rupture 41 MPa ISO 527
Déformation à la rupture 12 % ISO 527
Résistance au choc Charpy (entaillé), +23°C 8 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 65 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 155 °C ISO 75-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.4 % Sim. to ISO 62
Absorption d'humidité 0.2 % Sim. to ISO 62
Masse volumique 1380 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 120 °C -
Pré-séchage - temps 3 - 6 h -
L'humidité de traitement ≤0.03 % -
Température du moule 60 - 100 °C -
Température - Zone d'alimentation 60 - 80 °C -
Zone 1 250 - 265 °C -
Température de la buse 265 - 280 °C -
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Modifié choc
Caractéristiques
Bas gauchissement
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.