Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ EX401 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ EX401:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Tritan EX401, specifically developed for the Infant Care market, is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are clarity, excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan EX401 meets infant care sterilization requirements via boiling water or microwave steam sterilization. This newgeneration copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents.

Tritan EX401 can be converted into parts using injection molding, injection stretch blow molding (ISBM), and extrusion blow molding techniques.

Tritan EX401 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Contact Eastman representative for details on global food contact regulatory clearances.




Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.006 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1620 MPa ISO 527
Contrainte d'écoulement 45 MPa ISO 527
Déformation au seuil d'écoulement 7 % ISO 527
Contrainte à la rupture 49 MPa ISO 527
Déformation à la rupture 130 % ISO 527
Module de flexion, 23°C 1530 MPa ISO 178
Résistance au choc Izod avec entaille, +23°C 66 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 14 kJ/m² ISO 180/1A
Température -40 °C -
ASTM Data
Module en traction 1585 MPa ASTM D 638
Module de traction d’élasticité 44 MPa ASTM D 638
Résistance de traction à la rupture 53.1 MPa ASTM D 638
Allongement d’élasticité 7 % ASTM D 638
Allongement à la rupture 140 % ASTM D 638
Module de flexion 1585 MPa ASTM D 790
Dureté Rockwell R 115 - ASTM D 785
Izod choc avec entaille, 1/8 in 650 J/m ASTM D 256
Izod choc avec entaille, bas température 126 J/m ASTM D 256
Température -40 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 66 psi 109 °C ASTM D 648
DTUL à 264 psi 92 °C ASTM D 648
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 1 % ASTM D 1003
Lumière á Transmittance 92 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Densité 1170 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 88 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 260 - 282 °C -
Température du moule 38 - 66 °C -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Pré-séchage - température 88 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 240 - 250 °C -
Température du moule 25 - 45 °C -
Caractéristiques
Transformation
Moulage par injection, Soufflage
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur, Transparent, Stérilisable, Stérilisation à la vapeur
Caractéristiques
Amorphe, Copolymère
Résistance Chimique
Résistance chimique générale, Stabilité hydrolytique
Certifications
Contact alimentaire, FDA 21 CFR approbation
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.