Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TROGAMID® Care MX73 - PAPACM12 - Evonik Operations GmbH

Material Data Center offers the following functions for TROGAMID® Care MX73:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Trogamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Microcrystalline and transparent polyamides for for medical application

TROGAMID® Care MX is the material of choice for all applications dealing with pharmaceutical formulations, lipids or aggressive disinfectants, since it exhibits an exceptional resistance towards chemicals and stress-cracking. Examples include fluid and drug delivery equipment such as stop-cocks, dialyzer parts, housings, covers or hearing aids.
 
Target areas of application for TROGAMID® Care MX compounds include fluid and drug delivery systems, surgical instruments, housings, monitoring and imaging devices and durable medical equipment.
 
All advantages at a glance
- High transparency 
- High chemical resistance 
- Very good stress crack resistance
- UV resistance
- High dynamic load-bearing capacity
- High impact resistance
- Easy processability & colorability
- Free of BPA
- Gamma and EtO sterilizable

Biocompatibility of TROGAMID® Care
TROGAMID® Care grades were tested on biocompatibility for applications within the body of up to 30 days contact time and comply with USP <88> class VI and ISO 10993 standards.

Biocompatibility tests for TROGAMID® Care:


Processing of TROGAMID® Care
For information about processing of TROGAMID®, please follow the general commendations about “Processing of TROGAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 8.2 / * cm³/10min ISO 1133
Température 280 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 1400 / - MPa ISO 527
Contrainte d'écoulement 60 / - MPa ISO 527
Déformation au seuil d'écoulement 8 / - % ISO 527
Déformation nominale à la rupture >50 / - % ISO 527
Résistance au choc Charpy, +23°C N / - kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / - kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 14 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), -30°C 11 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Dureté Shore D 81 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 250 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 140 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 108 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 122 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 130 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 90 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 90 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.6 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3.2 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 115 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 325 / - E-4 IEC 62631-2-1
Résistivité transversale >1E13 / - Ohm*m IEC 62631-3-1
Rigidité diélectrique 27 / - kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 3.5 / * % Sim. to ISO 62
Absorption d'humidité 1.5 / * % Sim. to ISO 62
Masse volumique 1020 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion de plaques
Conditionnement
Granulés
Propriétés spéciales
Modifié choc, Stabilisé aux intempéries, Transparent, Stérilisable, Stérilisation par oxyde d'éthylène (EtO), Stérilisation par rayonnement gamma
Résistance Chimique
Résistance chimique générale, Fissuration à l’environnement
Certifications
Grade médical, Biocompatibility ISO 10993, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.