Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® S 4090 G6 - (PBT+ASA+PET)-GF30 - BASF

Material Data Center offers the following functions for Ultradur® S 4090 G6:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Low-warpage injection molding grade with 30 % glass fibres for technical parts, for which dimensional stability is very important (e.g.housings, plug-and-socket connectors).

Abbreviated designation according to ISO 1043: PBT ASA PET GF30
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 20 cm³/10min ISO 1133
Température 275 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.3 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 % ISO 294-4, 2577
ASTM Data
Retrait au moulage , parallèle 0.003 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 9700 MPa ISO 527
Contrainte à la rupture 125 MPa ISO 527
Déformation à la rupture 2.2 % ISO 527
Module de fluage en traction, 1h 7600 MPa ISO 899-1
Module de fluage en traction, 1000h 6700 MPa ISO 899-1
Résistance au choc Charpy, +23°C 58 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 50 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 7 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 6.5 kJ/m² ISO 179/1eA
ASTM Data
Module en traction 9653 MPa ASTM D 638
Résistance de traction à la rupture 125 MPa ASTM D 638
Allongement à la rupture 2.2 % ASTM D 638
Module de flexion 8274 MPa ASTM D 790
Résistance à la flexion 194 MPa ASTM D 790
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 223 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 175 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 210 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 160 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 25 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 105 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
ASTM Data
DTUL à 66 psi 210 °C ASTM D 648
DTUL à 264 psi 177 °C ASTM D 648
Température de fusion 223 °C ASTM D 3418
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.8 - IEC 62631-2-1
Permittivité relative, 1MHz 3.7 - IEC 62631-2-1
Facteur de pertes, 100Hz 30 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 180 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E14 Ohm IEC 62631-3-2
Rigidité diélectrique 39 kV/mm IEC 60243-1
Indice de résistance au cheminement 500 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.4 % Sim. to ISO 62
Absorption d'humidité 0.2 % Sim. to ISO 62
Masse volumique 1470 kg/m³ ISO 1183
Densité 1380 kg/m³ ASTM D 792
Propriétés spécifiques à la matièreValeurUnitéNorme du test
ISO Data
Indice de viscosité 105 cm³/g ISO 307, 1157, 1628
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 120 °C -
Pré-séchage - temps 4 h -
L'humidité de traitement ≤0.04 % -
Température de la matière fondue 250 - 275 °C -
Température du moule 60 - 100 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Module de cisaillement dynamique / Température , Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Contrainte / Déformation , Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Module sécant / Déformation , Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Contrainte / Déformation (isochrone) 23°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Module de fluage / Temps 23°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Courbe de fluage 23°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Contrainte / Déformation (isochrone) 40°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Module de fluage / Temps 40°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Courbe de fluage 40°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Contrainte / Déformation (isochrone) 60°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Module de fluage / Temps 60°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Courbe de fluage 60°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Contrainte / Déformation (isochrone) 80°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Module de fluage / Temps 80°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Courbe de fluage 80°C, Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Module de traction / Température , Ultradur® S 4090 G6, (PBT+ASA+PET)-GF30, BASF
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant
Propriétés spéciales
Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 270 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 80 °C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.