Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2640 Z6 R01 AT - (POM+PUR) - BASF

Material Data Center offers the following functions for Ultraform® N2640 Z6 R01 AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.

Abbreviated designation according to ISO 1043-1: POM-HI
Designation according to ISO 29988-POM-K,,M-GNPR,2-1
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 4.5 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 1.5 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.5 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1500 MPa ISO 527
Contrainte d'écoulement 40 MPa ISO 527
Déformation au seuil d'écoulement 15 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Module de fluage en traction, 1h 825 MPa ISO 899-1
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 18 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 9 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 165 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 70 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 130 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 110 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 140 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.5 - IEC 62631-2-1
Permittivité relative, 1MHz 4.3 - IEC 62631-2-1
Facteur de pertes, 100Hz 100 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 250 E-4 IEC 62631-2-1
Résistivité transversale 1E11 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E12 Ohm IEC 62631-3-2
Rigidité diélectrique 36 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 1 % Sim. to ISO 62
Absorption d'humidité 0.3 % Sim. to ISO 62
Masse volumique 1340 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 100 °C -
Pré-séchage - temps 3 h -
L'humidité de traitement ≤0.2 % -
Température de la matière fondue 190 - 215 °C -
Température du moule 60 - 80 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de cisaillement dynamique / Température , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte / Déformation , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module sécant / Déformation , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 23°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de fluage / Temps 23°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Courbe de fluage 23°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 40°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de fluage / Temps 40°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Courbe de fluage 40°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 60°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de fluage / Temps 60°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Courbe de fluage 60°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 80°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de fluage / Temps 80°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Courbe de fluage 80°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 100°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de fluage / Temps 100°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Courbe de fluage 100°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 120°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de fluage / Temps 120°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Courbe de fluage 120°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Volume spécifique (pvT) , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Module de traction / Température , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Caractéristiques
Copolymère
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 215 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.