Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® W2320 003 UN Q600 - POM - BASF

Material Data Center offers the following functions for Ultraform® W2320 003 UN Q600:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Very free-flowing, rapidly solidifying grade for use where processing is extremely difficult but mechanical properties are lower.

Abbreviated designation according to ISO 1043-1: POM
Designation according to ISO 29988-POM-K,,M-GNR,5-2
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 25 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 2.0 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.9 % ISO 294-4, 2577
Température d'éjection 110 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2750 MPa ISO 527
Contrainte d'écoulement 63 MPa ISO 527
Déformation au seuil d'écoulement 8.5 % ISO 527
Déformation nominale à la rupture 27 % ISO 527
Module de fluage en traction, 1h 2000 MPa ISO 899-1
Module de fluage en traction, 1000h 1350 MPa ISO 899-1
Résistance au choc Charpy, +23°C 170 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 150 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 4.5 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 4 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 166 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 95 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 156 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 150 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 110 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Yellow Card disponible oui - -
Aptitude à l'allumage 15 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.8 - IEC 62631-2-1
Permittivité relative, 1MHz 3.8 - IEC 62631-2-1
Facteur de pertes, 100Hz 10 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 65 E-4 IEC 62631-2-1
Résistivité transversale 1E12 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E15 Ohm IEC 62631-3-2
Rigidité diélectrique 40 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.8 % Sim. to ISO 62
Absorption d'humidité 0.2 % Sim. to ISO 62
Masse volumique 1410 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 200 °C ISO 294
Injection, température du moule 90 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Fonctions
Viscosité / Vitesse de cisaillement , Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultraform® W2320 003 UN Q600, POM, BASF
Module de cisaillement dynamique / Température , Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte / Déformation , Ultraform® W2320 003 UN Q600, POM, BASF
Module sécant / Déformation , Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte / Déformation (isochrone) 23°C, Ultraform® W2320 003 UN Q600, POM, BASF
Module de fluage / Temps 23°C, Ultraform® W2320 003 UN Q600, POM, BASF
Courbe de fluage 23°C, Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte / Déformation (isochrone) 40°C, Ultraform® W2320 003 UN Q600, POM, BASF
Module de fluage / Temps 40°C, Ultraform® W2320 003 UN Q600, POM, BASF
Courbe de fluage 40°C, Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte / Déformation (isochrone) 60°C, Ultraform® W2320 003 UN Q600, POM, BASF
Module de fluage / Temps 60°C, Ultraform® W2320 003 UN Q600, POM, BASF
Courbe de fluage 60°C, Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte / Déformation (isochrone) 80°C, Ultraform® W2320 003 UN Q600, POM, BASF
Module de fluage / Temps 80°C, Ultraform® W2320 003 UN Q600, POM, BASF
Courbe de fluage 80°C, Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte / Déformation (isochrone) 100°C, Ultraform® W2320 003 UN Q600, POM, BASF
Module de fluage / Temps 100°C, Ultraform® W2320 003 UN Q600, POM, BASF
Courbe de fluage 100°C, Ultraform® W2320 003 UN Q600, POM, BASF
Contrainte / Déformation (isochrone) 120°C, Ultraform® W2320 003 UN Q600, POM, BASF
Module de fluage / Temps 120°C, Ultraform® W2320 003 UN Q600, POM, BASF
Courbe de fluage 120°C, Ultraform® W2320 003 UN Q600, POM, BASF
Volume spécifique (pvT) , Ultraform® W2320 003 UN Q600, POM, BASF
Module de traction / Température , Ultraform® W2320 003 UN Q600, POM, BASF
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 185 - 230 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.