Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA11 black CF - PA11-CF - BASF

Material Data Center offers the following functions for Ultrasint PA11 black CF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9 / * cm³/10min ISO 1133
Température 220 / * °C -
Charge 2.16 / * kg -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 202 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 151 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 189 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, A 193 / * °C ISO 306
Température de ramolliss. Vicat, B 188 / * °C ISO 306
Propriétés diversessec / condUnitéNorme du test
Masse volumique 1070 / - kg/m³ ISO 1183
Bulk density 540 kg/m³ -
3D Datasec / condUnitéNorme du test
Other Standards[S]
Module en traction, flat 5900 / 4550 MPa ISO 527
Module en traction, upright 2500 / 2000 MPa ISO 527
Résistance à la traction, flat 82 / 71 MPa ISO 527
Résistance à la traction, upright 55 / 48 MPa ISO 527
Déformation à la rupture, flat 7 / 11 % ISO 527
Déformation à la rupture, upright 11 / 17 % ISO 527
Module de flexion, flat 5800 / 5000 MPa ISO 178
Module de flexion, upright 2500 / 2100 MPa ISO 178
Résistance au choc Charpy, +23°C, flat 54 / 63 kJ/m² ISO 179/1eU
Résistance au choc Charpy, +23°C, upright 33 / 51 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C, flat 6.4 / 6.7 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), +23°C, upright 4.7 / 4.7 kJ/m² ISO 179/1eA
Résistance au choc Izod, +23°C, flat 48 / 52 kJ/m² ISO 180/1U
Résistance au choc Izod, +23°C, upright 34 / 45 kJ/m² ISO 180/1U
Résistance au choc Izod avec entaille, +23°C, flat 8.7 / 8.5 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille, +23°C, upright 5 / 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Caractéristiques
Transformation
Additive Manufacturing, Frittage laser
Conditionnement
Poudre, Noir
Propriétés spéciales
Conductivité électrique accrue, Modifié choc
Résistance Chimique
Résistance chimique générale, Résistance aux huiles
Certifications
Contient des ressources renouvelables
Applications
Automobile, Électrotechnique et électrique
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.