Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® Care M40 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® Care M40 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
High viscosity, unreinforced polyether ether ketone designed for the medical device industry

VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days.

VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment.

VESTAKEEP® Care M40 G is a high viscosity, unreinforced polyether ether ketone for injection molding and extrusion. The semi-crystalline polymer features superior thermal and chemical resistance.

Biocompatibility of VESTAKEEP® Care
In an extensive testing program run by independent certified labs, biocompatibility has been tested following United States Pharmacopeia and ISO 10933-1:2003 guidelines.
The test reports attest VESTAKEEP® Care’s excellent biocompatibility.

Biocompatibility tests for VESTAKEEP® Care:


Processing of VESTAKEEP® Care
VESTAKEEP® Care resins can be processed using all conventional melt processing techniques such as injection moulding, extrusion, and compression moulding.

VESTAKEEP® Care M40 G can be processed by common machines for thermoplastics. We recommend a melt temperature between 370°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

Our technical experts would appreciate to give you support regarding the special requirements for the processing of VESTAKEEP® Care M40 G.

Delivery of VESTAKEEP® Care
VESTAKEEP® Care M40 G is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.
Pigmentation may affect values.
The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a
statistical evaluation. Therefore they must not be used to establish specifications.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY 

 
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 11 cm³/10min ISO 1133
Température 380 °C -
Charge 5 kg -
Retrait au moulage, parallèle 0.9 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.1 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3500 MPa ISO 527
Contrainte d'écoulement 96 MPa ISO 527
Déformation au seuil d'écoulement 5 % ISO 527
Déformation nominale à la rupture 30 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 7 kJ/m² ISO 179/1eA
Type de défaillance C - -
Résistance au choc Charpy (entaillé), -30°C 6 kJ/m² ISO 179/1eA
Type de défaillance C - -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, B 305 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 60 E-6/K ISO 11359-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 2.8 - IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Indice de résistance au cheminement 200 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.4 % Sim. to ISO 62
Masse volumique 1300 kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Conditionnement
Granulés
Caractéristiques
Stabilité thermique
Résistance Chimique
Résistance chimique générale
Certifications
Grade médical, Biocompatibility ISO 10993, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com