Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7293 BK 9.7507 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7293 BK 9.7507:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

High viscosity, plasticized, impact modified, heat- and light-stabilized polyamide 12 compound

VESTAMID® X7293 BK 9.7507 is a plasticized polyamide 12 compound with heat and light stabilizer for the extrusion of flexible tubing and hose, especially for automotive applications according to DIN 73378, (PA 12-HIPHL, Type 1), ISO/DIN 7628-1 (PA 12-HIPEHL, Type 1) and SAE J844.

VESTAMID® X7293 BK 9.7507 is distinguished by an easy processing as well as by a high impact strength at low temperatures.

Properties of compounds based on Polyamide 12 vary little with changing humidity due to low moisture absorption. Parts made of this semicrystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance.

VESTAMID® X7293 BK 9.7507 is supplied as cylindrical granules, ready for use, in moisture-proof bags.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 53 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 0.9 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.2 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 410 / 400 MPa ISO 527
Contrainte d'écoulement 26 / 24 MPa ISO 527
Déformation au seuil d'écoulement 32 / 32 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 120 / 125 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 7 / 6 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 172 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 13 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 45 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 100 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 130 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 180 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 180 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 11 / 12 - IEC 62631-2-1
Permittivité relative, 1MHz 4.6 / 3.7 - IEC 62631-2-1
Facteur de pertes, 100Hz 2000 / 1470 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 1900 / 1450 E-4 IEC 62631-2-1
Résistivité transversale 1E10 / 2.7E9 Ohm*m IEC 62631-3-1
Rigidité diélectrique - / 37 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.3 / * % Sim. to ISO 62
Absorption d'humidité 0.5 / * % Sim. to ISO 62
Masse volumique 1020 / - kg/m³ ISO 1183
Fonctions
Contrainte / Déformation , VESTAMID® X7293 BK 9.7507 (sec), PA12-I, Evonik
Module sécant / Déformation , VESTAMID® X7293 BK 9.7507 (sec), PA12-I, Evonik
Module de traction / Température , VESTAMID® X7293 BK 9.7507 (sec), PA12-I, Evonik
Caractéristiques
Transformation
Moulage par injection, Extrusion de tubes, Extrusion de profilés, Extrusion (autres)
Conditionnement
Granulés, Noir
Additifs
Lubrifiant, Plastifiant
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé à la chaleur
Caractéristiques
Grade tribologique
Résistance Chimique
Résistance chimique générale
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.