Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9057 OR E20081 - PA12 FR(30+40) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9057 OR E20081:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Low-viscosity, self-extinguishing PA12 Compound, free of halogen, PA12 FR(30 40)

VESTAMID® LX9057 OR E20081 is a heat- stabilized compound with an efficient halogen-free flame retardant. Tested according to UL94, it complies with the flammability classification V-2.

The halogen-free formulation makes VESTAMID® LX9057 OR E20081 especially suitable for the electronic and cable industry.

VESTAMID® LX9057 OR E20081 can be used for injection molding as well as for wire extrusion coating.

The semi-crystalline compounds based on PA12 only absorb small amounts of water. Therefore manufactured parts exhibit excellent dimensional stability at changing ambient humidity, constant high toughness, low coefficient of friction and good chemical resistance.
  
Due to the presence of flame retardant the melt temperature should not exceed 240°C. We recommend melt temperatures of 200°C-220°C.
 
VESTAMID® LX9057 OR is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 45 / * cm³/10min ISO 1133
Température 220 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.9 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.0 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 1200 / 820 MPa ISO 527
Contrainte d'écoulement 37 / 33 MPa ISO 527
Déformation au seuil d'écoulement 12 / 17 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C 130 / N kJ/m² ISO 179/1eU
Type de défaillance C / - - -
Résistance au choc Charpy, -30°C 69 / 122 kJ/m² ISO 179/1eU
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), +23°C 3 / 7 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 3 / 2 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 176 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 55 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 130 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 136 / * °C ISO 306
Inflammabilité ep. nom. 1.5 mm V-2 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité pr. épaisseur h V-2 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Yellow Card disponible oui / * - -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.5 / 7.5 - IEC 62631-2-1
Permittivité relative, 1MHz 3.2 / 3.5 - IEC 62631-2-1
Facteur de pertes, 100Hz 920 / 1920 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz - / 537 E-4 IEC 62631-2-1
Résistivité transversale 7.4E11 / 9.3E9 Ohm*m IEC 62631-3-1
Rigidité diélectrique 35 / 36 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.8 / * % Sim. to ISO 62
Absorption d'humidité 0.8 / * % Sim. to ISO 62
Masse volumique 1080 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Enduction
Conditionnement
Granulés
Propriétés spéciales
Ignifugé, Sans halogène, Stabilisé à la chaleur
Caractéristiques
Grade tribologique
Résistance Chimique
Résistance chimique générale
Applications
Électrotechnique et électrique
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.