Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9112 BK - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9112 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Conductive, heat-stabilized and light-resistant polyamide 12 compound for the extrusion coating of steel tubing

VESTAMID® LX9112 BK is a heat-stabilized, conductive polyamide 12 compound, especially developed for the pore-free extrusion coating of steel tubing.
 
Compared to commonly use conductive extrusion compounds VESTAMID® LX9112 BK is distinguished by a significant lower melt viscosity and respectively by outstanding extrusion characteristics even in very thin coatings.
 
Steel tubing coated with VESTAMID® LX9112 BK meet the requirements of the US automotive industry to prevent electrostatic charge caused by flowing liquid fuels.

Due to the excellent impact strength and the  good abrasion and chemical resistance of polyamide 12 the seamless coating with VESTAMID® LX9112 BK improves the corrosion resistance of steel tubing significantly.
 
VESTAMID® LX9112 BK is supplied as cylindrical pellets, ready for processing in moisture-proof packaging.


The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 34 / * cm³/10min ISO 1133
Température 240 / * °C -
Charge 10 / * kg -
Retrait au moulage, parallèle 1.2 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.5 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 2120 / 1690 MPa ISO 527
Contrainte d'écoulement 54 / 48 MPa ISO 527
Déformation au seuil d'écoulement 4 / 13 % ISO 527
Déformation nominale à la rupture 32 / >50 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 4 / 3 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 3 / 3 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 176 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 44 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 52 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 150 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 156 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 105 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 124 / * E-6/K ISO 11359-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 43000 / 29000 Ohm*m IEC 62631-3-1
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.11 / * % Sim. to ISO 62
Absorption d'humidité 0.65 / * % Sim. to ISO 62
Masse volumique 1120 / - kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 240 °C ISO 294
Injection, température du moule 60 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Caractéristiques
Transformation
Extrusion (autres), Enduction
Conditionnement
Granulés, Noir
Propriétés spéciales
Conductivité électrique accrue, Antistatique, Modifié choc, Stabilisé à la lumière, Stabilisé à la chaleur
Résistance Chimique
Résistance chimique générale
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.