Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9117 BK - PA12-(GF+CD) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9117 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Electrically polyamide 12 compound for quick connectors

VESTAMID® LX9117 BK 
is a glass-fiber-reinforced, electrically conductive PA12 molding compound that was developed in particular for the injection molding of connecting elements for fuel line systems (such as quick connectors).
 
The electrical conductivity of VESTAMID® LX9117 BK changes only slightly on contact with fuels, even if they contain alcohol. This is of great importance for use in fuel-conducting systems.
 
The material also has the advantageous properties characteristic of polyamide 12. The low water absorption leads to good dimensional stability of components in changing ambient humidity, and the other properties also remain virtually unchanged.
 
VESTAMID® LX9117 BK is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Our technical experts would appreciate to give you support regarding the special requirements for the processing of VESTAMID® LX9117 BK.
 
The use of colorants may change property values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
 
The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.3 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 7930 / - MPa ISO 527
Contrainte d'écoulement 127 / - MPa ISO 527
Déformation au seuil d'écoulement 4 / - % ISO 527
Déformation nominale à la rupture 4 / - % ISO 527
Résistance au choc Charpy, +23°C 70 / - kJ/m² ISO 179/1eU
Type de défaillance C / - - -
Résistance au choc Charpy, -30°C 50 / - kJ/m² ISO 179/1eU
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), +23°C 10 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), -30°C 9 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 177 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 40 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 169 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 179 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 173 / * °C ISO 306
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.1 / * % Sim. to ISO 62
Absorption d'humidité 0.6 / * % Sim. to ISO 62
Masse volumique 1330 / - kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 250 °C ISO 294
Injection, température du moule 80 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Caractéristiques
Transformation
Moulage par injection, Coulage
Conditionnement
Granulés, Noir
Additifs
Agent de démoulage
Propriétés spéciales
Conductivité électrique accrue, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.