Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra DS16 - PA1010 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra DS16:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Medium-viscosity polyamide 1010

VESTAMID® Terra DS16 NC is a medium-viscosity PA 1010 basic polymer. VESTAMID® Terra DS16 is semi-crystalline, which is the reason for its high mechanical resistance and chemical stability. It absorbs only little water. As a result its mechanical properties vary little when exposed to changing environmental humidity, and the material features a high dimensional stability.
 
VESTAMID® Terra DS16 can be used to manufacture films with good transparency.

The high melting point of VESTAMID Terra DS16 compounds results in a high heat deflection temperature that can be advantageous for some applications.
 
VESTAMID® Terra DS16 occupies a position between the high-performance long-chain polyamides such as PA 12 and PA 1212 and the standard polyamides PA 6 and PA 66, which have a shorter chain length.

VESTAMID® Terra DS16 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
 
VESTAMID® Terra is a group of new poly­amides, the monomers for which are based entirely or partly on renewable raw materials.

VESTAMID® Terra DS is the polycondensation product of 1,10-decamethylene diamine (D) and 1,10-dodecanedioic acid (sebacic acid-S). Because both monomers are extracted from castor oil, VESTAMID® Terra DS is based on natural, bio-based and renewable resources up to 100%.

The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 1.4 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.5 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 1700 / 1250 MPa ISO 527
Contrainte d'écoulement 54 / 48 MPa ISO 527
Déformation au seuil d'écoulement 5 / 22 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 7 / 7 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 7 / 5 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 200 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 37 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 55 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 136 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 171 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 115 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 135 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.6 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3.1 / - - IEC 62631-2-1
Résistivité transversale >1E13 / 8.3E11 Ohm*m IEC 62631-3-1
Rigidité diélectrique 37 / - kV/mm IEC 60243-1
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.8 / * % Sim. to ISO 62
Absorption d'humidité 1.4 / * % Sim. to ISO 62
Masse volumique 1040 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion (autres)
Conditionnement
Granulés, Grains
Propriétés spéciales
Stabilisé à la chaleur, Transparent
Résistance Chimique
Résistance chimique générale
Certifications
Contient des ressources renouvelables
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.