Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 47H NT - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 47H NT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Vydyne 47H NT is general-purpose, medium impact-modified, heat stabilized PA66 resin. The product offers improved resistance to thermal degradation.

47H NT is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline. 47H NT is designed to meet the critical low-temperature impact requirements called out in many automotive specifications.

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 1.8 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.6 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 2800 / 1700 MPa ISO 527
Contrainte d'écoulement 60 / 45 MPa ISO 527
Contrainte à la rupture 52 / 40 MPa ISO 527
Déformation à la rupture 22 / 60 % ISO 527
Module de flexion, 23°C 2300 / 780 MPa ISO 178
Résistance à la flexion 70 / 24 MPa ISO 178
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 19 / 62 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 17 / 24 kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 18 / 44 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 16 / 24 kJ/m² ISO 180/1A
Température -30 °C -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 260 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 63 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 185 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 111 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 136 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Glow Wire Flammability Index (GWFI) 700 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 775 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 700 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 725 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 725 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 0.75 mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 1E9 / - Ohm*m IEC 62631-3-1
Rigidité diélectrique 12 / - kV/mm IEC 60243-1
Indice de résistance au cheminement 525 / - - IEC 60112
ASTM Data
Résistance à l’arc 90 / - s ASTM D 495
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.2 / * % Sim. to ISO 62
Absorption d'humidité 2.3 / * % Sim. to ISO 62
Masse volumique 1100 / - kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 4 h -
Température de la matière fondue 285 - 305 °C -
Température du moule 65 - 95 °C -
Zone 1 280 - 310 °C -
Zone 2 280 - 310 °C -
Zone 3 280 - 310 °C -
Température de la buse 280 - 310 °C -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur
Résistance Chimique
Résistance chimique générale, Résistance aux solvants, Résistance aux huiles
Applications
Automobile, Électrotechnique et électrique, General Purpose
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com