Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Akromid T - PPA - Akro-Plastic GmbH

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Akromid T" in Material Data Center leads to the following information:

Tradename: Akromid T
Family: PPA
Producer: Akro-Plastic GmbH
40 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
AKROMID® T5 GF 50 6 black (8000) PPA-GF50
AKROMID® T5 GF 35 4 black (7692) PPA-GF35
AKROMID® T5 GF 40 4 black (7585) PPA-GF40
AKROMID® T5 GF 50 black (6247) PPA-GF50
AKROMID® T5 GF 50 9 black (8001) PPA-GF50
AKROMID® T9 CGM 15/10 S1 black (7850) PPA-(CF+GF)25
AKROMID® T9 GF 15 S1 black (7820) PPA-GF15
AKROMID® T9 GF 30 FR natural (7778) PPA-GF30
AKROMID® T9 GF 30 S1 black (7873) PPA-GF30
AKROMID® T9 GF 35 4 black (7858) PPA-GF35
AKROMID® T9 GF 40 4 black (7828) PPA-GF40
AKROMID® T9 GF 50 black (7601) PPA-GF50
AKROMID® T9 GF 50 black (7693) PPA-GF50
AKROMID® T9 M 40 black (7851) PPA-MX40
AKROMID® T5 GF 50 8 black (6205) PPA-GF50
AKROMID® T5 GF 20 8 black (6456) PPA-GF20
AKROMID® T5 GF 30 black (6485) PPA-GF30
AKROMID® T5 GF 30 8 black (6457) PPA-GF30
AKROMID® T5 GF 40 8 black (6458) PPA-GF40
AKROMID® T5 ICF 10 black (6772) PPA-CF10
AKROMID® T5 ICF 20 black (6773) PPA-CF20
AKROMID® T5 GF 40 black (6486) PPA-GF40
AKROMID® T5 8 black (6454) PPA
AKROMID® T5 GF 10 8 black (6455) PPA-GF10
AKROMID® T5 GF 30 6 black (8006) PPA-GF30
AKROMID® T5 GF 35 6 black (8004) PPA-GF35
AKROMID® T5 GF 35 6 natural (8005) PPA-GF35
AKROMID® T5 GF 35 natural (7162) PPA-GF35
AKROMID® T5 GF 40 6 black (8002) PPA-GF40
AKROMID® T5 GF 40 6 natural (8003) PPA-GF40
AKROMID® T5 GF 40 8 black (7963) PPA-GF40
AKROMID® T5 GF 50 natural (7834) PPA-GF50
AKROMID® T9 black (7953) PPA
AKROMID® T9 GF 15 S1 natural (7906) PPA-GF15
AKROMID® T9 GF 30 black (8315) PPA-GF30
AKROMID® T9 GF 30 grey (8134) PPA-GF30
AKROMID® T9 GF 50 6 black (7917) PPA-GF50
AKROMID® T9 ICF 20 6 black (7907) PPA-CF20
AKROMID® T9 ICF 30 6 black (7908) PPA-CF30
AKROMID® T9 ICF 40 6 black (7909) PPA-CF40

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.