Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Alathon® M5265 - (PE-HD) - LyondellBasell Industries

Material Data Center offers the following functions for Alathon® M5265:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Alathon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 6.5 g/10min ASTM D 1238
Temperatura 190 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Modulo a trazione 765 MPa ASTM D 638
Resistenza alla trazione di snervamento 26.4 MPa ASTM D 638
Resistenza alla trazione a rottura 27.6 MPa ASTM D 638
Allungamento a snervamento 12 % ASTM D 638
Allungamento a rottura 2230 % ASTM D 638
Modulo a flessione 1300 MPa ASTM D 790
Durezza D Shore 71 - ASTM D 2240
Resistenza all'urto Izod con intaglio, 1/8 in 64 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 69.4 °C ASTM D 648
Temperatura di fusione 132 °C ASTM D 3418
Temp.di rammollimento Vicat 127 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Densità 951 kg/m³ ASTM D 792
Bulk Density 609 kg/m³ -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche
Copolimero
Applicazioni
Imballaggio
Disponibilità geografica
Nord America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.