Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Apec® 1745 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Apec® 1745 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Apec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
  • MVR (330°C/2.16kg) 17 cm³/10 min
  • easy release
  • for superheated steam sterilization up to 143 °C
  • meets criteria of US Pharmacopeia (USP) Class VI
  • biocompatible according to many ISO 10993-1 test requirements
  • softening temperature (VST/B 120)=170 °C
  • Films for medical packaging
  • Contact lens holders
  • Medical vessels
  • Safety valve for respiration aids
  • Syringe tops
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 17 cm³/10min ISO 1133
Temperatura 330 °C -
Carico 2.16 kg -
Indice di Fluiditá, MFI 17 g/10min ISO 1133
Temperatura 330 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 0.8 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.8 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2400 MPa ISO 527
Carico unitario a trazione 70 MPa ISO 527
Deformazione a snervamento 6.8 % ISO 527
Deformazione nominale a rottura >50 % ISO 527
Modulo a flessione, 23°C 2400 MPa ISO 178
Resistenza all'urto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N kJ/m² ISO 179/1eU
Ball indentation hardness 120 MPa ISO 2039-1
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 148 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 161 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 170 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 65 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 65 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Indice di ossigeno 25 % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 2 mm -
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 2.9 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 10 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 80 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale >1E15 Ohm IEC 62631-3-2
Rigidità dielettrica 35 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 250 - IEC 60112
Proprietà OtticheValoreUnitáNorma del test
ISO Data
Trasmittanza luminosa 88[1] % ISO 13468-1, -2
Other Standards[S]
Indice di rifrazione 1.58 - ISO 489
1: Clear transparent materials  S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.3 % Sim. alla ISO 62
Assorbimento d'umidità 0.12 % Sim. alla ISO 62
Massa volumica 1170 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 330 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 100 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 130 °C -
Pre-essiccamento - Tempo 2 - 3 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 320 - 340 °C -
Temperatura dello stampo 110 - 130 °C -
Zona 1 290 - 300 °C -
Zona 2 300 - 310 °C -
Zona 3 310 - 320 °C -
Temperatura dell ugello 320 - 330 °C -
Contropressione 5 - 15 MPa -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Additivi
Agente di distacco
Caratteristiche speciali
Stabilizzato o stabile al calore, Trasparente, Sterilizzabile, Sterilizzazione a vapore
Certifications
Contiene risorse rinnovabili, Grado medico, Biocompatibility ISO 10993, Approvazione della USP class VI, ISCC Plus
Applicazioni
Medicale, Imballaggio
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.