Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Armlen" in Material Data Center leads to the following information:

Tradename: Armlen
Family: PP
Producer: R&P Polyplastic
83 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Armlen® PP GF 20-1EX PP-GF20
Armlen® PP GF 30-5HS PP-GF30
Armlen® PP MF 20-2HS PP-MF20
Armlen® PP MF 40-1 PP-MF40
Armlen® PP-2FR PP
Armlen® PE-2AFX PE
Armlen® PO MD 70-2FRX PO-MX70
Armlen® PP 7IM-901 (PP+PE)-X10
Armlen® PP 11IM-9001 PP
Armlen® PP 17IM PP
Armlen® PP E/P 15-1X PP
Armlen® PP E/P 15-2LS PP
Armlen® PP E/P 15-3 PP
Armlen® PP E/P 15-5MLS PP
Armlen® PP E/P 20-2 PP
Armlen® PP E/P 20-3 PP
Armlen® PP E/P 20-4MLS PP
Armlen® PP E/P 20-5M PP
Armlen® PP GF 10-1HS PP-GF10
Armlen® PP GF 10-2HS PP-GF10
Armlen® PP GF 20-1MEX PP-GF20
Armlen® PP GF 20-2LS PP-GF20
Armlen® PP GF 20-2EX PP-(GF+MX)25
Armlen® PP GF 25-1IM PP-GF25
Armlen® PP GF 30-1EX PP-GF30
Armlen® PP GF 30-2HS PP-GF30
Armlen® PP GF 30-3 PP-GF30
Armlen® PP GF 30-4HS PP-GF30
Armlen® PP GF 30-6HS-9010 PP-GF30
Armlen® PP GF 40-6HS-9010 PP-GF40
Armlen® PP GF 50-6HS PP-GF50
Armlen® PP GF MD 30-1 PP-GF30
Armlen® PP MD 10-1 PP-MD10
Armlen® PP MD 10-2LS PP-MD10
Armlen® PP MD 15-1FR PP-MD15
Armlen® PP MD 20-1 PP-MD20
Armlen® PP MD 40-2TS PP-MD40
Armlen® PP MD 40-3M PP-MD40
Armlen® PP MD 40-4HS-901 PP-MD40
Armlen® PP MD 40-4M PP-MD40
Armlen® PP MD 40-5TS PP-MD40
Armlen® PP MD 40-6TS PP-MD40
Armlen® PP MD 40-8.1TS PP-MD40
Armlen® PP MD 40-11TS PP-MD40
Armlen® PP MD 45-10D PP-MD45
Armlen® PP MD 50-2TS PP-MD50
Armlen® PP MD 50-5TS PP-MD50
Armlen® PP MF 10-1FRX PP-MF10
Armlen® PP MF 13-8IM PP-MF10
Armlen® PP MF 15-1FR PP-MF15
Armlen® PP MF 15-3FR PP-MF15
Armlen® PP MF 15-5IM-901 PP-MF15
Armlen® PP MF 20-2 PP-MF20
Armlen® PP MF 20-3-901 PP-MF20
Armlen® PP MF 20-3IM PP-T20
Armlen® PP MF 20-5IM PP-MF20
Armlen® PP MF 20-7IM PP-MF20
Armlen® PP MF 20-15IM PP-T20
Armlen® PP MF 20-18IM PP-MF20
Armlen® PP MF 25-1 PP-MF25
Armlen® PP MF 25-2TS PP-MF25
Armlen® PP MF 25-3-901 PP-MF25
Armlen® PP MF 30-1 PP-MF30
Armlen® PP MF 30-3IM PP-MF30
Armlen® PP MF 30-3TS PP-MF30
Armlen® PP MF 30-4IM PP-MF30
Armlen® PP MF 40-2M PP-MF40
Armlen® PP MF 35-1 PP-MF35
Armlen® PP TPE-11-90A-9010 TPE
Armlen® PP TPE 11-40D TPE
Armlen® PP TPE-10-70A TPE-MX
Armlen® PP TPE-10-75A TPE-MX
Armlen® PP TPE-17-J-80A TPE-MX
Armlen® PP-1EX PP
Armlen® PP-1FRX PP
Armlen® PP-2FRX PP
Armlen® PP-2IM PP
Armlen® PP-3FRX PP
Armlen® PP-3IM PP
Armlen® PP-4EX PP
Armlen® PP-4FRX PP
Armlen® PP-10IM-901 PP
Armlen® PP-12IM-8945 PP

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.