Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 5101-15 - PC-GX10 - Trinseo

Material Data Center offers the following functions for CALIBRE™ 5101-15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 15 g/10min ISO 1133
Temperatura 300 °C -
Carico 1.2 kg -
Ritiro di stampaggio, parallelo 0.3 % ISO 294-4, 2577
ASTM Data
Indice di fluidità a caldo, MFI 15 g/10min ASTM D 1238
Temperatura 300 °C -
Carico 1.2 kg -
Ritiro di stampaggio, parallelo 0.0035 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3380 MPa ISO 527
Carico unitario a trazione 62 MPa ISO 527
Carico unitario a rottura 61 MPa ISO 527
Deformazione a rottura 6 % ISO 527
Modulo a flessione, 23°C 3170 MPa ISO 178
Resistenza all'urto Izod, +23°C 29 kJ/m² ISO 180/1U
ASTM Data
Modulo a trazione 3378 MPa ASTM D 638
Resistenza alla trazione di snervamento 62.1 MPa ASTM D 638
Resistenza alla trazione a rottura 60.7 MPa ASTM D 638
Allungamento a rottura 6 % ASTM D 638
Modulo a flessione 3172 MPa ASTM D 790
Resistenza alla flessione 93.8 MPa ASTM D 790
Durezza Rockwell R 122 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 80.1 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 134 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 160 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm V-2 class IEC 60695-11-10
Spessore provato 1.6 mm -
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 3.2 mm -
Indice di ossigeno 32 % ISO 4589-1/-2
ASTM Data
UL 94 combustibilitá V-2 - UL 94
Spessore testati 1.59 mm -
coefficiente d’espansione termica, lung. 37.8 E-6/K ASTM D 696
DTUL a 264 psi 134 °C ASTM D 648
Temp.di rammollimento Vicat 160 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.25 % Sim. alla ISO 62
Massa volumica 1270 kg/m³ ISO 1183
Assorbimento d’acqua, 24hr 0.15 % ASTM D 570
Assorbimento d’acqua, equilibrio 0.25 % ASTM D 570
Densità 1270 kg/m³ ASTM D 792
Caratteristiche
Additivi
Agente di distacco
Caratteristiche speciali
Stabilizzato o stabile al calore
Applicazioni
IT / Apparecchiature per ufficio, Medicale
Disponibilità geografica
Nord America, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.