Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 603-2 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ 603-2:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 1.8 g/10min ISO 1133
Temperatura 300 °C -
Carico 1.2 kg -
ASTM Data
Indice di fluidità a caldo, MFI 1.8 g/10min ASTM D 1238
Temperatura 300 °C -
Carico 1.2 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2400 MPa ISO 527
Carico unitario a trazione 63 MPa ISO 527
Deformazione a snervamento 6.3 % ISO 527
Carico unitario a rottura 51 MPa ISO 527
Deformazione a rottura 50 % ISO 527
Modulo a flessione, 23°C 2400 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 69 kJ/m² ISO 179/1eA
ASTM Data
Modulo a trazione 2351 MPa ASTM D 638
Resistenza alla trazione di snervamento 63 MPa ASTM D 638
Resistenza alla trazione a rottura 51 MPa ASTM D 638
Allungamento a snervamento 6.3 % ASTM D 638
Allungamento a rottura 50 % ASTM D 638
Modulo a flessione 2399 MPa ASTM D 790
Resistenza alla flessione 93.1 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 801 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 127 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 140 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 146 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.6 mm -
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 1.6 mm -
DTUL a 66 psi 140 °C ASTM D 648
DTUL a 264 psi 127 °C ASTM D 648
Temp.di rammollimento Vicat 146 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1200 kg/m³ ISO 1183
Densità 1200 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Estrusione Profilati, Estrusione di Lastre/Fogli
Caratteristiche speciali
Estab. agli U.V. o per applicaz.in esterni
Caratteristiche
Resistenza del fuso
Disponibilità geografica
Europa, Asia Oceano Pacifico, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com