Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PA66-GF40-02P11/15 - PA66-GLF40 - Celanese

Material Data Center offers the following functions for CELSTRAN® PA66-GF40-02P11/15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 13700 / 10000 MPa ISO 527
Carico unitario a rottura 190 / 160 MPa ISO 527
Deformazione a rottura 1.6 / 2 % ISO 527
Resistenza all'urto Charpy, +23°C 40 / 45 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 41 / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 23 / 18 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 23 / - kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 261 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 255 / * °C ISO 75-1/-2
Temp.di inflessione sotto caricor, 8.00 MPa 240 / * °C ISO 75-1/-2
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica - / 1460 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 4 h -
Temperatura di fusione 300 - 315 °C -
Temperatura dello stampo 90 - 120 °C -
Funzioni
Sforzi-deformazione , CELSTRAN® PA66-GF40-02P11/15 (Secco), PA66-GLF40, Celanese
Sforzi-deformazione , CELSTRAN® PA66-GF40-02P11/15 (cond.), PA66-GLF40, Celanese
Modulo secante-deformazione , CELSTRAN® PA66-GF40-02P11/15 (Secco), PA66-GLF40, Celanese
Modulo secante-deformazione , CELSTRAN® PA66-GF40-02P11/15 (cond.), PA66-GLF40, Celanese
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Profilati, Estrusione di Lastre/Fogli, Altre Estrusioni, Soffiaggio, Stampaggio a Trasferimento
Forma fisica disponibile
Pellet
Additivi
Lubrificanti
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Long fiber reinforced
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
It is recommended to dry in a dehumidifying dryer: 4 hours at 80 °C.

During the processing of CELSTRAN it is important to watch and
control melt shear, for excessive shear reduces fiber length and
mechanical performance as well.

Processing recommendation:

- Conventional 3 zone screw, screw diameter minimum 40 mm
- Design flow channels for low melt shear
- Back pressure and screw rotation to realize a continous
plastification performance and thus a homogeneous melt.
- Apply higher temperature settings than for short fiber compounds

Melt temperature (in the screw anteroom) 300-315 °C
Mold surface temperature 90-120 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.