Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PP-GF20-0553 Black - PP-GLF20 - Celanese

Material Data Center offers the following functions for CELSTRAN® PP-GF20-0553 Black:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Material code according to ISO 1043-1: PP Polypropylene copolymer reinforced with 20weight percent long glass fibers.Black.  Low emission. The fibers are chemically coupled to the polypropylene matrix. The pellets are cylindrical and normally as well as the embedded fibers 11 mm long. Parts molded of CELSTRAN have outstanding mechanical properties such as high strength and stiffness combined with high heat deflection. The notched impact strength is increased at elevated and low temperatures due to the fiber skeleton built in the parts. The long fiber reinforcement reduces creep significantly. The very isotropic shrinkage in the molded parts minimizes the warpage. Complex parts can be manufactured with high reproducibility by injection molding. Application field: Functional/structural parts for automotive

Flammability at thickness h (1 mm)HB-
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.4 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.5 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 4700 MPa ISO 527
Carico unitario a rottura 84 MPa ISO 527
Deformazione a rottura 2.5 % ISO 527
Resistenza all'urto Charpy, +23°C 56 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 60 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 20 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 20 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 159 °C ISO 75-1/-2
Temp.di inflessione sotto caricor, 8.00 MPa 136 °C ISO 75-1/-2
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 1.0 mm -
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1030 kg/m³ ISO 1183
Funzioni
Sforzi-deformazione , CELSTRAN® PP-GF20-0553 Black, PP-GLF20, Celanese
Modulo secante-deformazione , CELSTRAN® PP-GF20-0553 Black, PP-GLF20, Celanese
Sforzi-deformazioni (isocrona) 23°C, CELSTRAN® PP-GF20-0553 Black, PP-GLF20, Celanese
Modulo di scorrimento-tempo 23°C, CELSTRAN® PP-GF20-0553 Black, PP-GLF20, Celanese
Curva di scorrimento 23°C, CELSTRAN® PP-GF20-0553 Black, PP-GLF20, Celanese
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Nero
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Rafforzamento accoppiato chimicamente, Resistenza al scorrimento, Long fiber reinforced, Low Emission, Bassa deformazione, Copolimero
Applicazioni
Automotive
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.