Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Chemlon® 280 - PA6 - Teknor Apex Co.

Material Data Center offers the following functions for Chemlon® 280:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Chemlon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.0175 mm/mm ASTM D 955
Ritiro di stampaggio, perpend. 0.0225 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione 41.4 MPa ASTM D 638
Allungamento a snervamento 7 % ASTM D 638
Allungamento a rottura 150 % ASTM D 638
Modulo a flessione 1620 MPa ASTM D 790
Resistenza alla flessione 55.2 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 1170 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 294 J/m ASTM D 256
Temperatura -40 °C -
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 0.813 mm -
DTUL a 66 psi 135 °C ASTM D 648
DTUL a 264 psi 51.7 °C ASTM D 648
Temperatura di fusione 217 °C ASTM D 3418
Indice limite di ossigeno 20 % ASTM D 2863
Proprietà ElettricheValoreUnitáNorma del test
ASTM Data
Rigidità elettrica, breve periodo di tempo 10 kV/mm ASTM D 149
Resistenza di volume 1010 Ohm*cm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Assorbimento d’acqua, 24hr 0.8 % ASTM D 570
Densità 1070 kg/m³ ASTM D 792
Caratteristiche
Caratteristiche speciali
Alto urto o modificato all'urto
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.