Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Diakon ST15G6 - PMMA - Lucite International

Material Data Center offers the following functions for Diakon ST15G6:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Diakon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 13 g/10min ISO 1133
Ritiro di stampaggio, parallelo 0.4 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.7 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Resistenza a trazione 70 MPa ISO 527
Deformazione a rottura 6 % ISO 527
Modulo a flessione, 23°C 2400 MPa ISO 178
Resistenza all'urto Charpy, +23°C 21 kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 2.1 kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 2.1 kJ/m² ISO 180/1A
Durezza Rockwell M 78 - ISO 2039-2
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 88 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 97 °C ISO 306
Temp.di rammollimento Vicat, B 91 °C ISO 306
Reazione al fuoco a spessore h HB class IEC 60695-11-10
ASTM Data
coefficiente d’espansione termica, lung. 80 E-6/K ASTM D 696
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1 % ASTM D 1003
Trasmissione luminosa 91.5 % ASTM D 1003
Indice di rifrazione 1.49 - ASTM D 542
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.3 % Sim. alla ISO 62
Massa volumica 1180 kg/m³ ISO 1183
Densità 1180 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Caratteristiche speciali
Alto urto o modificato all'urto
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.