Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DOWLEX™ IP 10 - (PE-HD) - The Dow Chemical Company

Material Data Center offers the following functions for DOWLEX™ IP 10:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dowlex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 10 g/10min ASTM D 1238
Temperatura 190 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 29 MPa ASTM D 638
Resistenza alla trazione a rottura 18.6 MPa ASTM D 638
Allungamento a snervamento 7 % ASTM D 638
Allungamento a rottura 1200 % ASTM D 638
Durezza D Shore 55 - ASTM D 2240
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 81.1 °C ASTM D 648
Temperatura di fusione 132 °C ASTM D 3418
Temp.di rammollimento Vicat 130 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Densità 960 kg/m³ ASTM D 792
Caratteristiche
Forma fisica disponibile
Pellet, Bianco
Caratteristiche
Basso odore
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti 10/2011, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Applicazioni
Automotive
Disponibilità geografica
Nord America, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.