Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DuraStar™ DS2010 - PCTA - Eastman Chemical Co.

Material Data Center offers the following functions for DuraStar™ DS2010:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Durastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Durastar™ DS2010 polymer contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2010 has very good toughness as shown by Izod impact resistance. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS2010 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Under existing

United States Food and Drug Administration (FDA) regulations, Durastar™ DS2010 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240. This product is certified to ANSI/NSF Standard 51.




Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.004 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a trazione 47 MPa ISO 527
Deformazione a snervamento 4 % ISO 527
Carico unitario a rottura 49 MPa ISO 527
Deformazione a rottura 210 % ISO 527
Modulo a flessione, 23°C 1750 MPa ISO 178
Resistenza alla flessione 64 MPa ISO 178
Resistenza all'urto Izod con intaglio, +23°C 29.6 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 6.3 kJ/m² ISO 180/1A
Temperatura -40 °C -
Energia di perforazione, +23°C 71 J ISO 6603-2
ASTM Data
Resistenza alla trazione di snervamento 46 MPa ASTM D 638
Resistenza alla trazione a rottura 53.1 MPa ASTM D 638
Allungamento a snervamento 5 % ASTM D 638
Allungamento a rottura 310 % ASTM D 638
Modulo a flessione 1900 MPa ASTM D 790
Durezza Rockwell 105 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 370 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 60 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 66 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 73 °C ISO 75-1/-2
ASTM Data
UL 94 combustibilitá V-2 - UL 94
Spessore testati 3 mm -
DTUL a 66 psi 73 °C ASTM D 648
DTUL a 264 psi 65 °C ASTM D 648
Proprietà ElettricheValoreUnitáNorma del test
ASTM Data
Rigidità elettrica, breve periodo di tempo 16.6 kV/mm ASTM D 149
Fattore di dissipazione dielèttrica, 1 MHz 0.015 - ASTM D 150
Costante dielèttrica, 1 MHz 2.5 - ASTM D 150
Resistenza superficiale 1E17 Ohm ASTM D 257
Resistenza di volume 1E17 Ohm*cm ASTM D 257
Resistenza all’arco 123 s ASTM D 495
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 0.3 % ASTM D 1003
Trasmissione luminosa 91 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1190 kg/m³ ISO 1183
Densità 1200 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 70 °C -
Pre-essiccamento - Tempo 3 h -
Temperatura di fusione 250 - 290 °C -
Temperatura dello stampo 15 - 30 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Colore naturale
Additivi
Agente di distacco
Caratteristiche speciali
Alto urto o modificato all'urto, Trasparente
Resistenza Chimica
Resistenza chimica generale, Resistenza all’olio
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR, Approvato per l'utilizzo per contatto con alimenti secondo la NSF 51
Applicazioni
Imballaggio, Attrezzature sportive
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com