Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN058 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN058:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastar™ EN058 Copolyester is a copolymer PET. It is crystallized and has an lntrinsic Viscosity of 0.58. Eastar™ EN058 copolyester is tailored to meet the need of the injection-molded cosmetics and personal care market.

Eastar™ EN058 is crystallized to allow faster, high-temperature drying. Its high-flow characteristics allow faster cycle times.




Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.002 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 58 MPa ASTM D 638
Resistenza alla trazione a rottura 24 MPa ASTM D 638
Allungamento a snervamento 4 % ASTM D 638
Allungamento a rottura 90 % ASTM D 638
Modulo a flessione 2400 MPa ASTM D 790
Durezza Rockwell R 111 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 56 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 33 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 69 °C ASTM D 648
DTUL a 264 psi 63 °C ASTM D 648
Temp.di rammollimento Vicat 80 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1 % ASTM D 1003
Trasmissione luminosa 82 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Assorbimento d’acqua, 24hr 0.19 % ASTM D 570
Densità 1330 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 160 °C -
Pre-essiccamento - Tempo 4 - 6 h -
Temperatura di fusione 277 - 293 °C -
Temperatura dello stampo 16 - 32 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Colore naturale
Caratteristiche
Copolimero
Certifications
Contatto con gli alimenti
Applicazioni
Automotive, Elettrotecnica ed electrici, Imballaggio, Attrezzature sportive
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.