Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ AN014 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ AN014:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastar™ AN014 copolyester is a high flow product that contains a mold release. Other outstanding features of Eastar™ are easily maintained such as excellent appearance and clarity, good physical properties, chemical resistance, and easy processing. Eastar™ AN014 is approved for food contact. Eastar™ AN014 flow lengths are increased 20-40% relative to Eastar™ AN004 as shown by spiral flow testing. This high flow product is especially suited for those applications utilizing thin-walled intricate tools. Under existing United States Food and Drug Administration (FDA) regulations, Eastar™ AN014 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.




Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.003 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 50 MPa ASTM D 638
Resistenza alla trazione a rottura 43 MPa ASTM D 638
Allungamento a snervamento 5 % ASTM D 638
Allungamento a rottura 270 % ASTM D 638
Modulo a flessione 1900 MPa ASTM D 790
Durezza Rockwell 107 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 80.1 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 44 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 73 °C ASTM D 648
DTUL a 264 psi 66 °C ASTM D 648
Temp.di rammollimento Vicat 86 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1 % ASTM D 1003
Trasmissione luminosa 92 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Assorbimento d’acqua, 24hr 0.15 % ASTM D 570
Densità 1190 kg/m³ ASTM D 792
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 70 °C -
Pre-essiccamento - Tempo 4 h -
Temperatura di fusione 230 - 280 °C -
Temperatura dello stampo 15 - 30 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Profilati
Forma fisica disponibile
Colore naturale
Additivi
Agente di distacco
Caratteristiche speciali
Trasparente
Caratteristiche
Copolimero
Resistenza Chimica
Resistenza chimica generale
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Applicazioni
Imballaggio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.