Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® T90D - Copolyester - SK Chemicals

Material Data Center offers the following functions for ECOZEN® T90D:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

ECOZEN® is a glycol-modified polyethylene terephthalate (PETG) with exceptional

transparency and chemical resistance.

Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.0025 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a trazione 44.6 MPa ISO 527
Deformazione a snervamento 5 % ISO 527
Carico unitario a rottura 48.1 MPa ISO 527
Deformazione a rottura 204 % ISO 527
Modulo a flessione, 23°C 1830 MPa ISO 178
Resistenza alla flessione 65.1 MPa ISO 178
Resistenza all'urto Izod con intaglio, +23°C 74 kJ/m² ISO 180/1A
ASTM Data
Resistenza alla trazione di snervamento 43.7 MPa ASTM D 638
Resistenza alla trazione a rottura 44.1 MPa ASTM D 638
Allungamento a snervamento 5.5 % ASTM D 638
Allungamento a rottura 360 % ASTM D 638
Modulo a flessione 1687 MPa ASTM D 790
Resistenza alla flessione 62.8 MPa ASTM D 790
Durezza Rockwell R 107 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 65 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 76 °C ISO 75-1/-2
ASTM Data
DTUL a 66 psi 75 °C ASTM D 648
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1 % ASTM D 1003
Trasmissione luminosa 90 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Densità 1240 kg/m³ ASTM D 792
Caratteristiche
Caratteristiche speciali
Stabilizzato o stabile al calore, Trasparente
Caratteristiche
Copolimero
Resistenza Chimica
Resistenza chimica generale
Certifications
Contiene risorse rinnovabili, Contatto con gli alimenti, RoHS
Applicazioni
Imballaggio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.