Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Fibrolon® 3D Wood - (PLA+Copolyester)-W... - FKuR Kunststoff GmbH

Material Data Center offers the following functions for Fibrolon® 3D Wood:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Fibrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Biodegradable polymer compound suitable for the production of 3D printing filaments. The biobased carbon content is > 75 % (calculated). Contains wood fibers.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 3.1 cm³/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Indice di Fluiditá, MFI 3.5 g/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2900 MPa ISO 527
Resistenza a trazione 47 MPa ISO 527
Deformazione a snervamento 5 % ISO 527
Carico unitario a rottura 38 MPa ISO 527
Deformazione a rottura 6.5 % ISO 527
Modulo a flessione, 23°C 2950 MPa ISO 178
Resistenza all'urto Charpy, +23°C 21 kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 4.4 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 155 °C ISO 11357-1/-3
Altre ProprietàValoreUnitáNorma del test
Biobased content 75 % -
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Type of extrusion profile - -
Pre-essiccamento - Temperatura 60 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Umidità del Processo ≤0.2 % -
Temperatura - Zona di Alimentazione 60 °C -
Zona 1 160 °C -
Zona 2 170 °C -
Zona 3 180 °C -
Zona 4 180 °C -
Temperatura dell ugello 185 °C -
Caratteristiche
Processabilità e Forma di Forni
Estrusione Profilati, Additive Manufacturing
Forma fisica disponibile
Pellet, Marrone
Certifications
Contiene risorse rinnovabili, Biodegradabile
Applicazioni
Filament for 3D Printing, Giocattoli
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.